Harmonised or product standard

    EN 1504-6 - Products and systems for the protection and repair of concrete structures - part 6: anchoring of reinforcing steel bar

    Testing · NAC-037-TL

    In short

    EN 1504-6 - Products and systems for the protection and repair of concrete structures - part 6: anchoring of reinforcing steel bar. For concrete repair and protection products, Amstelfy covers anchoring of reinforcing steel bar in its ISO/IEC 17025-accredited laboratory (NAC-037-TL). Reports and certificates are written for use in CE marking files, Declarations of Performance and third-party approvals across Europe.

    What the standard covers

    EN 1504-6 is the harmonised standard for products used to anchor reinforcing bars into existing concrete so that the bar develops its force: cementitious and polymer mortars and resins placed in drilled holes around ribbed bars. The standard demonstrates the product's anchoring capability through two benchmark tests on a standard bar and concrete rather than through a full design characterisation. Pull-out resistance to EN 1881 requires that the displacement of the bar under a load of 75 kN does not exceed 0.6 mm. Creep under sustained load to EN 1544 requires that the displacement under a continuous 50 kN load for three months does not exceed 0.6 mm. Further characteristics are chloride ion content, glass transition temperature for polymer products, corrosion behaviour and, where relevant, reaction to fire and dangerous substances.

    Type testing and factory production control

    Ribbed bars are anchored with the product in holes drilled in reference concrete blocks following the manufacturer's installation instructions and cured for the stated time. In the pull-out test the bar is loaded in tension in steps while its displacement relative to the concrete is measured, up to and beyond 75 kN, and the load–displacement curve is recorded to failure. For the creep test a sustained load of 50 kN is held for three months with displacement readings at increasing intervals. Chloride content is determined to EN 1015-17 and the glass transition temperature of resins to EN 12614. The client specifies the embedment conditions and product type tested.

    What the report states

    The report gives the displacement at 75 kN and the ultimate pull-out behaviour of each specimen, the creep displacement curve and the value at the end of the sustained load period, chloride content against the 0.05 % limit for cementitious products and the measured Tg against the standard's minimum for polymer products. The pass–fail outcome against 0.6 mm is stated explicitly for the DoP.

    Where the result is required

    CE marking of anchoring grouts and resins for starter bars, dowels and connections in repair and extension works under EN 1504-9 principle 4, method 4.3, bonding bar reinforcement in drilled holes. Where the designer needs bond values for post-installed rebar design to EN 1992-1-1 across embedment depths, concrete classes and conditions, the product is assessed under EAD 330087 and the resulting ETA, which EN 1504-6 does not replace.

    What we assess

    • anchoring of reinforcing steel bar

    Products covered

    • concrete repair and protection products

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by a harmonised European standard are CE marked on the basis of a Declaration of Performance; other product standards support national approvals and third-party certification. Amstelfy provides the initial type testing / type testing and, where the standard is on its ISO/IEC 17065 scope, acts as the product certification body.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    EN 1504-6 confirms that the product anchors a bar within fixed displacement limits in two benchmark tests and leads to CE marking. An ETA under EAD 330087 characterises bond strength for design, with embedment depths, concrete classes, temperatures, drilling methods and durability, and is what a structural engineer needs to size a post-installed rebar connection.

    Polymer anchoring materials can continue to displace under sustained load, especially at elevated temperature. Holding 50 kN for three months and limiting the displacement to 0.6 mm screens out products that would let the bar slip over the life of the repair. Cementitious products are tested the same way.

    The displacement of the bar at a load of 75 kN must not exceed 0.6 mm, measured relative to the concrete surface. The ultimate load is recorded as well, but the acceptance criterion in the standard is the displacement limit, not a minimum failure load.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing