US qualification standard

    ASTM C234 - Standard test method for comparing concretes on the basis of the bond developed with reinforcing steel

    Testing · NAC-037-TL

    In short

    ASTM C234 - Standard test method for comparing concretes on the basis of the bond developed with reinforcing steel. Amstelfy's laboratory in Amstelveen performs this ASTM method for concrete with rebar: bond strength. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM C234 determines

    ASTM C234 compares concretes, not reinforcing bars, on the basis of the bond they develop with a deformed steel bar. A single bar is embedded in a concrete specimen and pulled out while the slip of the bar relative to the concrete is measured at the loaded end and at the free end. Bond stress is computed from the pull-out load and the embedded bar surface at specified slips and at the maximum load. Because specimens are cast with the bar in both horizontal and vertical positions, the method also exposes the effect of bleeding and settlement under top-cast bars. ASTM has withdrawn the method as a current standard; it remains in use as a comparative pull-out procedure where a specification or research programme calls for it.

    Specimens, conditioning and procedure

    Concretes to be compared are batched with the same bar type and embedment, with companion cylinders for ASTM C39 so results can be related to compressive strength. Cube specimens are cast around the bar, some with the bar horizontal and some with the bar vertical, and cured moist to the agreed age. Each specimen is seated on a bearing plate in a testing machine, the projecting bar is gripped, and load is applied at a controlled rate while dial gauges or transducers record loaded-end and free-end slip. Loading continues to the maximum load or until the bar yields or the concrete splits.

    What the report states

    The report presents, for each concrete and casting position, the load–slip curves, the bond stress at the specified free-end and loaded-end slips, the maximum bond stress and the failure mode, pull-out, splitting or bar yield, together with the companion cylinder strength. Ratios between the candidate concrete and the reference concrete are the comparative outcome.

    Where the result is required

    Admixture, cement and fibre suppliers use it to show that a modified concrete bonds to reinforcement at least as well as a reference mix, for example when introducing a new water reducer, a lightweight aggregate or a self-consolidating mix in markets working to ACI 318 and ASTM specifications. It complements beam-end tests to ASTM A944 and the European pull-out and beam tests of EN 10080, which focus on the bar rather than the concrete.

    What we assess

    • bond strength

    Products covered

    • concrete with rebar

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    No. It ranks concretes relative to one another under identical bar and embedment conditions. Development lengths in ACI 318 come from the code equations, and bar-specific bond qualification uses beam-end or beam tests. Treat the result as a comparative index for the concrete.

    Bond under a horizontal bar depends on how much the fresh concrete bleeds and settles beneath it, which a vertical bar does not show. Testing both positions reveals whether a candidate mix, for instance a high-slump or retarded concrete, loses bond on top-cast bars.

    The reference and candidate mix designs or delivered materials, the bar size and grade to be used in every specimen, the test age, and the slips at which bond stress should be reported if the project specification differs from the method. Bars from one heat are used throughout.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing