    ASTM C143/C143M - Standard test method for slump of hydraulic-cement concrete. Amstelfy's laboratory in Amstelveen performs this ASTM method for fresh concrete: slump. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM C143/C143M determines

    ASTM C143/C143M measures the slump of fresh hydraulic-cement concrete as a single-number index of consistency. A truncated cone 300 mm high with a 200 mm base and 100 mm top is filled and compacted in a fixed way, lifted vertically, and the vertical settlement of the concrete relative to the mould height is the slump. The method covers plastic, cohesive concrete with coarse aggregate up to 37.5 mm; it is not applicable where the slump is below 15 mm or above 230 mm, nor to mixes that shear or collapse rather than subside. Slump reflects water content, admixture dosage and aggregate grading for a given mix and is the field control most purchasers specify.

    Specimens, conditioning and procedure

    A representative sample is taken under ASTM C172 and wet-sieved over the 37.5 mm sieve if larger aggregate is present. The dampened mould is held down on a flat, rigid, non-absorbent base and filled in three layers of approximately equal volume, each rodded 25 times with a 16 mm hemispherical-tipped tamping rod. The top is struck off, the mould is raised vertically in 5 ± 2 s without twisting, and the whole operation from filling to lifting is completed within 2.5 min. The slump is measured at the displaced original centre of the top surface. A falling-away or shearing-off of one side is recorded and the test repeated on a fresh portion.

    What the report states

    The report gives the slump to the nearest 5 mm, the sampling time and location, concrete temperature if measured and any wet-sieving. If two consecutive tests shear, the concrete is reported as lacking the plasticity and cohesiveness needed for the method. Results are compared with the slump and tolerance stated in the order or specification.

    Where the result is required

    Delivery acceptance under ASTM C94, field verification of mix designs for ACI 318 projects, batching uniformity checks and the fresh-property records that accompany specimens cast for ASTM C39 or C78. It is also the consistency check when fibres, admixtures or supplementary cementitious materials are being compared in laboratory trial batches before a US evaluation-report programme.

    What we assess

    • slump

    Products covered

    • fresh concrete

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The cone geometry is the same and both rod three layers 25 times, so values are broadly comparable. Differences lie in timing requirements, the reporting resolution, the treatment of shear failures and the consistency classes that EN 206 attaches to the result, so each report should name the method used.

    A shear, where one side slides away, invalidates the result and the test is repeated on another portion of the sample. Two consecutive shears mean the mix is not plastic and cohesive enough for the method. A full collapse indicates a slump beyond the range the method covers.

    Non-plastic, very stiff mixes below about 15 mm slump, very fluid mixes above 230 mm, self-consolidating concrete, which is measured by slump flow under ASTM C1611, and concrete with a significant fraction of aggregate above 37.5 mm unless it is wet-sieved first.