European Assessment Document

    EAD 330499-00-0601 - Bonded fasteners for use in concrete

    Testing · NAC-037-TLCertification · NAC-026-PPSETA route

    In short

    EAD 330499-00-0601 is the EOTA European Assessment Document for bonded fasteners for use in concrete. Amstelfy Technical Solutions tests bonded (chemical) anchors with threaded rods and rebars, injection systems and capsule systems against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): bond strength in cracked and uncracked concrete, installation conditions (dry, wet, flooded holes; temperature), sustained load and long-term behaviour and freeze-thaw and alkalinity durability. The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 330499-00-0601 covers bonded fasteners: injection or capsule systems in which a resin or cementitious mortar anchors a threaded rod, an internally threaded sleeve or a reinforcing bar in a drilled hole. Because the load path depends on the bond between mortar, steel and concrete, the central essential characteristic is the characteristic bond resistance τRk in cracked and uncracked concrete, reported per installation condition. The EAD assesses the system for defined use categories: the drilling method (hammer, diamond core, hollow drill bit, compressed air), the hole condition (dry, wet or water-filled), the installation temperature range and the service temperature ranges, each defined by a long-term and a short-term temperature. Resistance to sustained load, crack movement, high alkalinity and sulphurous atmosphere and, where claimed, seismic categories C1 and C2 complete the assessment; versions 01 and 02 keep the same structure.

    Assessment programme

    Each series uses the complete system: the cartridge or capsule, mixer, cleaning tools and steel element supplied by the manufacturer, installed by the laboratory in holes drilled as specified. Reference tension tests are confined so that bond rather than the concrete cone governs, in low- and high-strength concrete and in cracked slabs at the crack width prescribed by the EAD. Functioning tests vary what goes wrong on site: reduced hole cleaning, wet and flooded holes, installation at the lowest and highest permitted temperatures, installation direction, and shortened curing. Sustained-load tests run at ambient and at the maximum long-term service temperature with displacement logged against time; tests at elevated temperature give the bond reduction with temperature. Freeze-thaw cycles and alkaline storage address durability.

    What the report states

    The report lists per series the ultimate loads, bond stresses, displacements and failure modes (bond at the steel, bond at the concrete, cone, steel), the mean and 5 % fractile, and the ratio of each functioning series to its reference. The TAB turns these into τRk,ucr and τRk,cr per diameter, temperature range and installation category, the sustained-load factor, the installation parameters and the seismic values of the ETA.

    Where the result is required

    The ETA supports the design of bonded anchors with EN 1992-4 and CE marking of the system under AVCP system 1. It is the European counterpart of US qualification under ACI 355.4 and ICC-ES AC308, and the injection mortars assessed here are commonly assessed in parallel for post-installed rebar connections under EAD 330087. Typical products are epoxy, vinylester, hybrid and cementitious injection systems and glass or foil capsules for structural fixings, steel-to-concrete connections and retrofits.

    What we assess

    • bond strength in cracked and uncracked concrete
    • installation conditions (dry, wet, flooded holes; temperature)
    • sustained load and long-term behaviour
    • freeze-thaw and alkalinity durability
    • seismic categories C1/C2

    Products covered

    • bonded (chemical) anchors with threaded rods and rebars
    • injection systems
    • capsule systems

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Other versions on the scope: EAD 330499-01-0601; EAD 330499-02-0601

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    Yes, if both drilling methods are to appear in the ETA. Diamond coring leaves a smooth hole wall and the bond can drop markedly, so the EAD treats it as a separate installation category with its own reference and functioning tests. Hollow drill bits with dust extraction can usually be covered by a shorter comparison series against hammer drilling.

    Each range pairs a long-term temperature, which governs the sustained-load tests, with a short-term temperature for brief excursions. The manufacturer selects the ranges to be claimed and bond is tested at the upper temperatures, so one ETA may list different τRk values per range. Installation temperature is a separate parameter, fixed by the lowest temperature at which the mortar cures reliably.

    The EAD fixes a minimum test duration and a displacement that must not be exceeded, and the creep curve is extrapolated to the working life. The elevated-temperature series run in parallel with the ambient series, but both can only start once the reference tests have defined the load level, so they normally end last.

    Related standards

    All Anchors, fasteners & post-installed rebar testing