US qualification standard

    ASTM C1581/C1581M - Standard test method for determining age at cracking and induced tensile stress characteristics of mortar and concrete under restrained shrinkage

    Testing · NAC-037-TL

    In short

    ASTM C1581/C1581M - Standard test method for determining age at cracking and induced tensile stress characteristics of mortar and concrete under restrained shrinkage. Amstelfy's laboratory in Amstelveen performs this ASTM method for mortar and concrete: restrained shrinkage (ring test). Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM C1581/C1581M determines

    ASTM C1581/C1581M quantifies the tendency of a cementitious mixture to crack when its shrinkage is restrained. A ring of mortar or concrete is cast around an instrumented steel ring and allowed to dry from its outer circumference only. As the specimen shrinks it compresses the steel ring, and strain gauges on the inner surface of the steel record the build-up of tensile stress in the concrete. A sudden drop in strain marks the age at cracking. The rate at which stress develops before cracking and the net time to cracking are combined to classify the mixture's potential for cracking. The method is applicable to mixtures with a nominal maximum aggregate size of 13 mm or less.

    Specimens, conditioning and procedure

    The mixture is cast between the steel ring and an outer mould, consolidated, and kept covered. At 24 ± 1 h the outer ring is removed and the top surface is sealed so that moisture leaves only through the outer face. Specimens are stored at 23 ± 2 °C and 50 ± 4 % relative humidity, and the steel ring strain is recorded at least every 30 min from the start of drying. The test runs until cracking or until the agreed maximum age, commonly 28 days. Companion specimens for compressive or splitting strength can be cast from the same batch. Three ring specimens per mixture are the normal set.

    What the report states

    The report plots strain against age for each ring and states the age at cracking, the strain rate factor, the average stress rate in MPa per day and the net time to cracking, with the mixture classified into one of the four potential-for-cracking bands the method defines, from high to low. Uncracked rings at the end of the test are reported as such with their stress rate.

    Where the result is required

    Comparison of shrinkage-reducing and shrinkage-compensating admixtures, repair mortars and overlays, high-performance concretes and fibre-reinforced mixtures for US project specifications and ICC-ES submittals that call for a low cracking potential. It complements free drying shrinkage data from ASTM C157 and offers European producers a US-format counterpart to the restrained shrinkage and bond assessment of EN 12617-4 required under EN 1504-3.

    What we assess

    • restrained shrinkage (ring test)

    Products covered

    • mortar and concrete

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The concrete annulus is thin relative to normal structural sections, so large aggregate would dominate the cross-section and distort both stress development and crack formation. Mixtures with coarser aggregate must be wet-sieved or evaluated by another restrained shrinkage method, and the report states what was done.

    The mixture is reported as uncracked at the final age together with its average stress rate. A long time to cracking combined with a low stress rate places the mixture in the lowest cracking-potential band, which is often the client's objective for shrinkage-compensated or shrinkage-reduced products.

    Both restrain shrinkage, but EN 12617-4 applies a repair mortar to a concrete substrate and judges the outcome by bond and cracking of the layer, whereas C1581 measures stress build-up in a steel ring and the age at cracking. They answer different specifications and are not convertible.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing