US qualification standard

    ASTM C1579 - Standard test method for evaluating plastic shrinkage cracking of restrained fiber reinforced concrete

    Testing · NAC-037-TL

    In short

    ASTM C1579 - Standard test method for evaluating plastic shrinkage cracking of restrained fiber reinforced concrete. Amstelfy's laboratory in Amstelveen performs this ASTM method for fibre reinforced concrete: plastic shrinkage cracking. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM C1579 determines

    ASTM C1579 evaluates how well fibres reduce plastic shrinkage cracking in fresh concrete during the first hours after placing. A slab specimen is cast in a mould whose base carries a central raised stress riser and two smaller restraining ribs, so that shrinkage of the drying surface concentrates a crack above the riser. The specimen is placed, immediately after finishing, in an environmental chamber where temperature, humidity and air flow produce an evaporation rate of at least 1.0 kg/m² per hour from a free water surface. A control panel of the same concrete without fibres is tested alongside. The comparison of average crack widths gives the cracking reduction ratio, a measure of the fibre's effectiveness at the tested dosage.

    Specimens, conditioning and procedure

    Fibre-reinforced and control concretes are batched from the same materials, with fresh properties recorded, and panels are cast and finished in the standard moulds. The panels enter the chamber within the time the method allows and remain under the controlled drying conditions until the concrete has set and cracking has stabilised, with the evaporation rate verified on a pan of water. After the exposure period the crack over the stress riser is examined and its width measured at a series of points along its length with an optical device, and the average crack width is calculated for each panel. The time at which cracking is first observed is also recorded.

    What the report states

    The report gives the average crack width of the fibre panels and of the control panels, the evaporation rate and chamber conditions achieved, fresh concrete properties and the cracking reduction ratio, CRR, expressed in percent as one minus the ratio of fibre to control crack width. A higher CRR at a stated fibre dosage is the comparative performance indicator.

    Where the result is required

    Micro-synthetic and macro-synthetic fibre suppliers use CRR values to support dosage recommendations for slabs on grade, toppings and shotcrete, and in ICC-ES or project submittals where plastic shrinkage control is the claimed function of the fibre. It pairs with ASTM D7508 and ASTM C1116 for product qualification and gives European producers a US-format equivalent to the restrained plastic shrinkage evidence they hold for EN 14889-2 Class Ia and Ib fibres.

    What we assess

    • plastic shrinkage cracking

    Products covered

    • fibre reinforced concrete

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    It states by what percentage the average plastic shrinkage crack width was reduced compared with the identical plain concrete under the same drying conditions. It is specific to the fibre type, dosage and mix tested; it is not a guarantee that no cracks will form on site.

    Enough concrete for the fibre panels and the control panels cast in the same session, plus fresh-property tests. The client supplies the fibres at the dosages to be evaluated and agrees the mix design; aggregates and cement can be sourced locally to a specified grading.

    Plastic shrinkage cracking depends on the mix, bleeding and the exact drying conditions achieved in the chamber. Testing the plain concrete at the same time removes those variables, so the ratio between the two panels isolates the fibre's contribution rather than the day's conditions.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing