US qualification standard

    ASTM C1609 - Standard test method for flexural performance of fiber-reinforced concrete (beam with third-point loading)

    Testing · NAC-037-TL

    In short

    ASTM C1609 - Standard test method for flexural performance of fiber-reinforced concrete (beam with third-point loading). Amstelfy's laboratory in Amstelveen performs this ASTM method for fibre reinforced concrete: flexural performance, residual strength. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM C1609 determines

    ASTM C1609/C1609M characterises the post-cracking behaviour of fibre-reinforced concrete in bending. An unnotched beam is loaded at its third points under closed-loop control of the net mid-span deflection, so that the load drop after matrix cracking is captured instead of causing a sudden failure. From the load–deflection curve the method derives the first-peak strength, the peak strength and residual strengths at net deflections of 1/600 and 1/150 of the span, plus the toughness as the area under the curve to L/150. These parameters describe how much load the fibres carry across a crack at serviceability and ultimate deflection levels, which is the property that US specifications use to define fibre dosages for slabs, shotcrete and precast elements.

    Specimens, conditioning and procedure

    Beams of 100 × 100 × 350 mm tested on a 300 mm span or 150 × 150 × 500 mm on a 450 mm span are moulded, with external vibration preferred so fibre distribution is not disturbed, and moist-cured to the test age. Net deflection is measured with two transducers on a yoke attached at the neutral axis above the supports, averaging both sides to cancel seating and twisting. Loading proceeds at the slow controlled deflection rate the method specifies up to first crack and may be increased thereafter until the deflection reaches L/150. The machine must be stiff and servo-controlled; open-loop load control is not acceptable.

    What the report states

    For each beam the report gives first-peak load and strength, peak load and strength, residual loads and strengths at L/600 and L/150, toughness T150 in joules and the equivalent flexural strength ratio in percent, together with the full load–deflection curve, specimen dimensions and fibre dosage. For a 150 mm beam on a 450 mm span the two residual deflections are 0.75 mm and 3.0 mm.

    Where the result is required

    Specification and acceptance of steel, synthetic and hybrid fibre-reinforced concrete under ASTM C1116, ACI 544 and ACI 360 slab design, tunnel segment and shotcrete specifications, and ICC-ES evaluation reports for macro-synthetic and steel fibres. European fibre producers entering the US market have the beams tested in parallel with EN 14651 so that one casting programme serves both markets.

    What we assess

    • flexural performance, residual strength

    Products covered

    • fibre reinforced concrete

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    C1609 uses an unnotched beam in four-point bending controlled by mid-span deflection and reports residual strengths at deflection fractions of the span. EN 14651 uses a notched beam in three-point bending controlled by crack mouth opening and reports fR,1 to fR,4 at CMOD values. Numbers from one cannot be converted to the other.

    The 150 mm beam is the usual choice and the method requires it once fibre length or aggregate size exceeds the limits it sets for the small beam. The 100 mm beam suits short fibres and small aggregate but gives higher scatter and somewhat different values, so the size must be reported and kept constant within a programme.

    C1609 reports individual beams, so the number comes from the specification. Design guides and evaluation criteria typically ask for sets of at least three to five beams per dosage and mix, with companion cylinders for compressive strength, because residual strength scatter is higher than first-crack scatter.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing