European Assessment Document

    EAD 330087-01-0601 - Systems for post-installed rebar connections with mortar

    Testing · NAC-037-TLCertification · NAC-026-PPSETA route

    In short

    EAD 330087-01-0601 is the EOTA European Assessment Document for systems for post-installed rebar connections with mortar. Amstelfy Technical Solutions tests injection mortars for post-installed reinforcing bars against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): bond strength vs. cast-in rebar, installation in dry/wet/flooded holes and different drilling methods, sustained load, freeze-thaw, high-alkalinity and sulphurous atmosphere durability and fire resistance data support (where applicable). The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 330087-01-0601 assesses mortar systems used to anchor deformed reinforcing bars in drilled holes so that the connection can be designed as if the bar had been cast in, following the anchorage and lap-splice rules of EN 1992-1-1. The assessment does not produce an anchor resistance in the sense of EN 1992-4; it verifies that the bond and the load-slip behaviour of the post-installed bar are at least equivalent to a cast-in bar in the same concrete, and it fixes the conditions under which that equivalence holds. The essential characteristics are the bond strength relative to cast-in reinforcement, the admissible drilling methods and hole conditions, installation and service temperatures, the bar diameters and embedment lengths covered, resistance to sustained load, and the durability of the mortar under alkaline, sulphurous and freeze-thaw exposure. Fire resistance data can be added.

    Assessment programme

    Members are cast with reference bars placed before concreting, and companion holes are drilled for post-installed bars of the same diameter and embedment. Confined tension tests prevent concrete-cone failure so that bond governs; both series are loaded to failure and compared for strength and for the stiffness of the load-slip curve. Variants repeat the comparison for each drilling method claimed, for dry, wet and water-filled holes, for reduced hole cleaning, for the extreme installation temperatures and for the largest diameter at the deepest embedment. Sustained-load tests at ambient and at the maximum long-term temperature, freeze-thaw cycling of installed bars and exposure of mortar specimens to alkaline solution and to sulphur dioxide atmosphere complete the programme.

    What the report states

    For every series the report gives the bond stress at failure and at the displacement limits, the ratio to the cast-in reference, the failure mode and the statistical evaluation. The TAB uses the ratios to confirm the design bond strength fbd of EN 1992-1-1 or to set reduction factors, together with minimum cover and spacing, the maximum embedment depth and the installation instructions reproduced in the ETA.

    Where the result is required

    Post-installed rebar ETAs serve connections of new slabs, walls and columns to existing structures, closing of openings and seismic retrofit, designed with EN 1992-1-1; systems claiming improved bond-splitting behaviour use the EOTA TR 069 design method. The system is CE marked under AVCP system 1. Most mortars assessed here also hold an ETA as bonded anchors under EAD 330499, and the US route is the rebar development-length provisions of ICC-ES AC308.

    What we assess

    • bond strength vs. cast-in rebar
    • installation in dry/wet/flooded holes and different drilling methods
    • sustained load, freeze-thaw, high-alkalinity and sulphurous atmosphere durability
    • fire resistance data support (where applicable)

    Products covered

    • injection mortars for post-installed reinforcing bars

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    EAD 330499 produces anchor resistances for design to EN 1992-4, including concrete-cone and splitting checks and behaviour in cracked concrete. EAD 330087 shows that the mortar lets a deformed bar behave like cast-in reinforcement, so the connection is designed with the anchorage and lap rules of EN 1992-1-1 and the ordinary design bond strength. Many systems carry both ETAs.

    The EAD requires tests on a selection across the claimed range, with the smallest and largest diameters always included and the deepest embedment installed under the least favourable conditions to show that the mortar can be injected without voids. Intermediate diameters are covered by interpolation. Embedment lengths beyond those tested cannot be claimed in the ETA.

    Yes. The ETA can give bond stresses as a function of steel temperature for the fire design of the connection, derived from tests on heated bond specimens or from an assessment method accepted by the TAB. If fire data are wanted they should be planned with the main programme so that the same mortar batch and concrete are used.

    Related standards

    All Anchors, fasteners & post-installed rebar testing