US qualification standard

    ASTM E1512 - Standard test methods for testing bond performance of bonded anchors

    Testing · NAC-037-TL

    In short

    ASTM E1512 - Standard test methods for testing bond performance of bonded anchors. Amstelfy's laboratory in Amstelveen performs this ASTM method for bonded anchors: bond strength under temperature, moisture and sustained load conditions. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM E1512 determines

    ASTM E1512 complements ASTM E488 for anchors whose capacity depends on an adhesive. Where E488 measures strength under standard conditions, E1512 defines tests that expose the bond to the conditions that degrade it: elevated temperature of concrete and adhesive, moisture in the hole at installation, freeze-thaw cycling of installed anchors and long-term sustained load. The tests are run in tension with a confined set-up so that the bond, not the concrete cone, is the failure mode, and the results are expressed as bond stress over the embedded surface or as the ratio of the conditioned capacity to the unconditioned reference. The standard is a test method without acceptance limits; ICC-ES AC308 and ACI 355.4 call it up and set the limits.

    Specimens, conditioning and procedure

    Adhesive anchors are installed in concrete members with the manufacturer's cleaning, mixing and curing procedure, with reference specimens installed in clean dry holes. Elevated-temperature tests bring concrete and anchor to the target temperature, verified by thermocouples, and load them to failure while hot. Moisture tests install anchors in damp or water-saturated holes and in holes filled with water. Freeze-thaw specimens are installed, kept wet and cycled between the prescribed temperatures before testing. Sustained-load specimens carry a constant tension, a fraction of the mean reference capacity, at standard and at elevated temperature while displacement is recorded against time and the creep curve is extrapolated to the service life. All tension tests are confined and the loading rate follows the method.

    What the report states

    The report gives bond stress at failure and displacement for each specimen, the mean and coefficient of variation per series, the ratio of each conditioned series to the reference series and, for sustained-load tests, the displacement-time curves with the extrapolated displacement at the design life. The acceptance criteria that call the method use these ratios as reduction factors on the characteristic bond strength.

    Where the result is required

    ASTM E1512 results are required in adhesive anchor qualification under ACI 355.4 and in the ICC-ES AC308 test programme, where they define the temperature categories, the installation conditions covered by the evaluation report and the sustained-load reduction. They also serve manufacturers comparing adhesive formulations and specifiers checking a product for hot climates or wet substrates. The corresponding European series are part of EAD 330499 and EAD 330087.

    What we assess

    • bond strength under temperature, moisture and sustained load conditions

    Products covered

    • bonded anchors

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The concrete member or the zone around the anchor is heated until thermocouples at the embedment depth show the target temperature, which is held long enough for the adhesive to reach it, and the anchor is then loaded to failure at that temperature. The capacity ratio to the room-temperature reference gives the temperature reduction used by the acceptance criteria.

    A damp hole has been wetted and the free water removed; a water-saturated hole is drilled in concrete soaked for a defined period; a water-filled hole still contains standing water at installation. Each represents a site condition and each is a separate series, since adhesives react differently to moisture on the hole wall and to displacement of water by the injected product.

    An unconfined test would often fail by concrete breakout, which is governed by the concrete and the embedment rather than by the adhesive. By reacting the load close to the anchor the cone is suppressed and failure occurs at the adhesive interface, so the measured value is the bond stress that the qualification needs. Bond stress is calculated over the nominal embedded surface of the rod.

    Related standards

    All Anchors, fasteners & post-installed rebar testing