Test method

    EN 13970 - Flexible sheets for waterproofing - bitumen water vapour control layers

    Testing · NAC-037-TL

    In short

    EN 13970 - Flexible sheets for waterproofing - bitumen water vapour control layers. Amstelfy's laboratory determines water vapour transmission properties of bitumen vapour control layers according to EN 13970 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 13970 determines

    EN 13970 is the harmonised product standard for bitumen water vapour control layers, the sheets laid on the warm side of the thermal insulation of a flat or pitched roof to stop moisture from the building diffusing into the insulation. Its central characteristic is water vapour transmission, declared as the water vapour resistance factor or the equivalent air layer thickness sd determined by EN 1931, which for a bitumen vapour control layer is high. Around this the standard defines watertightness, tensile properties, resistance to tearing at the nail shank, joint strength, flexibility at low temperature, straightness, thickness and mass per unit area, visible defects, reaction to fire and the durability of water vapour transmission and watertightness after heat ageing. Conformity is shown by type testing and factory production control, and the manufacturer declares the values in the Declaration of Performance.

    Specimens, conditioning and procedure

    The type-testing programme starts with the vapour test: specimens are sealed over cups and the mass change is followed under the temperature and humidity gradient of EN 1931 until a steady rate is reached, and the sd value is calculated from thickness and transmission rate. In parallel, watertightness is tested by EN 1928, tensile properties by EN 12311-1, nail tear by EN 12310-1, joint shear by EN 12317-1 and cold flexibility by EN 1109, with dimensions, thickness, mass per unit area and visible defects taken from EN 1848-1, EN 1849-1 and EN 1850-1. Durability specimens are heat aged to EN 1296 and then retested for vapour transmission and watertightness. Factory production control repeats the main tests periodically.

    What the report states

    The report gives the water vapour transmission rate and the sd value in metres, or the resistance factor, with the test conditions, together with watertightness as pass or fail, tensile force in N per 50 mm and elongation, nail tear and joint forces in N, the cold-bend temperature, dimensions, mass per unit area and fire class, and the vapour and watertightness results after heat ageing. These are the declared characteristics for the Declaration of Performance.

    Where the result is required

    EN 13970 is the CE-marking standard for bitumen vapour control layers used under mineral wool, PIR and EPS insulation on flat roofs, including aluminium-laminated sheets for high-humidity buildings such as pools and food factories. Building physicists use the declared sd value in condensation calculations, and roofing contractors use the joint and tear values to choose between loose-laid, nailed and torch-bonded vapour control layers. Plastic vapour control layers are covered by EN 13984.

    What we assess

    • water vapour transmission properties

    Products covered

    • bitumen vapour control layers

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The cup method of EN 1931 measures the mass of water vapour passing through the sheet over time. A bitumen sheet with an aluminium foil lets through so little that the mass change is tiny and the test runs for weeks until the rate is steady. The resulting sd value in metres is what condensation calculations need, and the report states the test conditions used.

    The vapour control layer must survive installation, foot traffic before the insulation is laid and the nailing or bonding of the next layers; a torn or opened lap destroys its function. Tensile strength, nail tear and joint strength therefore appear in the standard, and watertightness shows that the sheet also acts as a temporary roof during construction.

    Rarely for the bitumen itself, but ageing can embrittle the sheet so that it cracks at laps and loses watertightness, and it can affect the bond of a laminated foil. The standard therefore requires vapour transmission and watertightness to be repeated after storage at elevated temperature to EN 1296, and the retained values are declared.

    Related standards

    All Waterproofing membranes, roof underlays & liquid-applied systems testing