Test method

    EN 12317-1 - Flexible sheets for waterproofing - shear resistance of joints - bitumen sheets

    Testing · NAC-037-TL

    In short

    EN 12317-1 - Flexible sheets for waterproofing - shear resistance of joints - bitumen sheets. Amstelfy's laboratory determines shear resistance of joints of bitumen sheets according to EN 12317-1 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 12317-1 determines

    EN 12317-1 determines the shear resistance of joints in bitumen waterproofing sheets: the maximum force a lap joint carries when the two bonded sheets are pulled in their own plane, the loading a seam sees when a membrane is stretched by substrate movement or wind suction. The specimen is a 50 mm wide strip containing the full overlap, and it is tested like a tensile specimen in EN 12311-1, at the same width and speed, so that the joint result can be compared directly with the tensile strength of the sheet. A sound joint fails outside the lap at a force close to the sheet strength; a weak joint slides apart in the bitumen or delaminates the carrier. The failure mode is therefore reported with the force, and both together show whether the bonding method is adequate.

    Specimens, conditioning and procedure

    Lap joints are made in the laboratory by the method of the manufacturer, with the overlap width used on site, and conditioned for the period the standard specifies. Strips 50 mm wide are cut perpendicular to the joint so that the overlap lies in the middle of the specimen. Each strip is clamped at the standard grip separation and pulled at a constant speed of 100 mm/min until failure. The maximum force is recorded, and the specimen is examined to classify the failure as sheet rupture outside the joint, shear within the bitumen, delamination from the carrier or separation at the surfacing. The direction of the sheet in the joint is noted.

    What the report states

    The report gives the shear resistance of the joint in N per 50 mm as the mean with individual values, the failure mode of each specimen and the bonding method and conditioning. Product standards ask the manufacturer to declare the value, which is read next to the tensile strength from EN 12311-1 to judge whether the joint or the sheet governs; both appear in the Declaration of Performance.

    Where the result is required

    Cited by EN 13707 for bitumen roofing sheets, EN 13969 for damp proofing and tanking sheets, EN 13970 for vapour control layers and EN 14695 for bridge-deck sheets, all of which declare joint strength because a membrane is only as tight as its laps. Manufacturers use it to qualify torching parameters and self-adhesive compounds, to check laps bonded over granules and to compare the sheet in both roll directions. Plastic and rubber sheets use EN 12317-2.

    What we assess

    • shear resistance of joints

    Products covered

    • bitumen sheets

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Because the specimen width and speed are the same as in EN 12311-1, the joint force can be set against the tensile force of the sheet. If the specimen breaks in the sheet outside the lap, the joint is stronger than the sheet and the bonding method is proven; if it fails in the lap at a lower force, the joint governs and the installation method needs attention.

    Joints are made with the overlap the manufacturer specifies for site use, so the result applies to that overlap. For bitumen sheets the force in shear rises with the bonded length only up to a point, after which the sheet itself fails, so a wider lap mainly adds safety against workmanship rather than strength. The report records the overlap tested.

    Product standards generally require the unaged value, but a manufacturer who wants to show durability of the seam can have joints heat aged to EN 1296 before the shear test, or tested at elevated temperature. Both are reported as additional tests with the conditions stated, and both are useful for self-adhesive sheets, whose bond develops and changes with time.

    Related standards