Test method

    EN 15820 - Polymer modified bituminous thick coatings - watertightness

    Testing · NAC-037-TL

    In short

    EN 15820 - Polymer modified bituminous thick coatings - watertightness. Amstelfy's laboratory determines watertightness of PMBC coatings according to EN 15820 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 15820 determines

    EN 15820 determines the watertightness of a polymer modified bituminous thick coating in the situation that matters on a basement: a dried film spanning a gap in the substrate while water presses on it. The coating is applied over a slot in a rigid substrate, cured, and then loaded on its outer face with water at a defined pressure for a defined period while the underside is open to inspection. Water passing through the film, through the bond at the slot edges or through the reinforcement is a failure. By testing at the pressure levels that EN 15814 assigns to each watertightness class, the method sorts coatings into W1, W2A and W2B. It complements crack bridging, which checks the span over a moving crack, by checking tightness under pressure.

    Specimens, conditioning and procedure

    A substrate with a slot of the width specified in the standard is prepared, and the coating is applied over it at the declared dry film thickness, including the reinforcement fleece where the system uses one, and cured under laboratory climate until fully dry. The specimen is clamped into a pressure vessel so that the coated face can be loaded with water. Pressure is raised to the level for the class claimed and held for the period the standard prescribes. The uncoated side is inspected for water, drops or damp patches at the slot. The test is repeated on the number of specimens the standard calls for, and the class is only awarded if all pass.

    What the report states

    The report states the test pressure and duration, the condition of the underside of each specimen and whether water passed, and the watertightness class that follows: W1, W2A or W2B as defined in EN 15814. Dry film thickness, reinforcement and curing period are recorded, since the class is valid only for that build-up. The class is declared in the Declaration of Performance.

    Where the result is required

    Required for the watertightness class in the Declaration of Performance under EN 15814 and the key class in national basement waterproofing rules, where the water load of the structure (soil moisture, non-pressing water, pressing water) determines the minimum class. Manufacturers also use it when adding a reinforcement fleece or increasing the recommended thickness to move a product from W2A to W2B. Sheet membranes use EN 1928 for the same property.

    What we assess

    • watertightness

    Products covered

    • PMBC coatings

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    A basement wall cracks and has joints, and that is where leaks start. Testing the coating over a slot reproduces an unsupported span under water pressure, so that the result reflects the weakest realistic situation rather than a film fully backed by concrete. The slot width is fixed by the standard so that results are comparable between laboratories.

    The classes differ in the water pressure applied, and in national rules in the water load they are matched to, with W2B the highest. A product tested only at the lower pressure receives the lower class; a manufacturer who wants W2B must have the specimens pass at the higher pressure. The declared class may not exceed what every specimen withstood.

    Yes, if the unreinforced build-up passes at the required pressure. Many systems need the fleece to bridge the slot under pressure, so the class is often tied to it. The report states exactly what was tested, and the Declaration of Performance should declare the class only for the build-up that passed.

    Related standards

    All Waterproofing membranes, roof underlays & liquid-applied systems testing