Harmonised or product standard

    EN 1504-7 - Products and systems for the protection and repair of concrete structures - part 7: reinforcement corrosion protection

    Testing · NAC-037-TL

    In short

    EN 1504-7 - Products and systems for the protection and repair of concrete structures - part 7: reinforcement corrosion protection. For concrete repair and protection products, Amstelfy covers reinforcement corrosion protection in its ISO/IEC 17025-accredited laboratory (NAC-037-TL). Reports and certificates are written for use in CE marking files, Declarations of Performance and third-party approvals across Europe.

    What the standard covers

    EN 1504-7 is the harmonised standard for coatings applied to cleaned reinforcing steel exposed during repair, before the repair mortar is placed. Two product types exist: active coatings, usually cement-based with corrosion-inhibiting pigments, which maintain passivity around the bar, and barrier coatings, usually epoxy, which isolate the steel from moisture, chlorides and oxygen. The coating must protect the steel without destroying the bond between bar and surrounding mortar, so the standard sets two performance requirements: corrosion protection, assessed by exposing coated bars to an aggressive environment and inspecting for corrosion, and shear adhesion, comparing the bond of coated bars in concrete with that of uncoated bars. Glass transition temperature applies to polymer coatings.

    Type testing and factory production control

    Bars are prepared to a defined cleanliness, coated at the manufacturer's thickness and cured. For the corrosion protection test to EN 15183 coated bars, with their ends sealed, are exposed in the corrosive conditions the method prescribes and afterwards examined for rust formation and coating defects; uncoated reference bars are exposed alongside to confirm the aggressiveness of the exposure. For shear adhesion to EN 15184 coated and uncoated bars are embedded in concrete, pulled out and the bond stresses compared. The glass transition temperature of polymer coatings is measured to EN 12614. The client states whether the product is active or barrier type.

    What the report states

    The report describes the condition of the coated bars after exposure with photographs and states whether corrosion occurred, gives the pull-out bond of coated bars as a percentage of the uncoated reference, which the standard requires to be at least 80 %, and the Tg where applicable. These results are declared in the DoP as corrosion protection and shear adhesion.

    Where the result is required

    CE marking of rebar primers and protective slurries used in EN 1504-9 principle 7, preserving or restoring passivity, and principle 11, control of anodic areas, in patch repairs on bridges, car parks, balconies and marine structures. Specifiers require EN 1504-7 compliance in repair systems together with an EN 1504-3 mortar and, where appropriate, an EN 1504-2 surface protection.

    What we assess

    • reinforcement corrosion protection

    Products covered

    • concrete repair and protection products

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by a harmonised European standard are CE marked on the basis of a Declaration of Performance; other product standards support national approvals and third-party certification. Amstelfy provides the initial type testing / type testing and, where the standard is on its ISO/IEC 17065 scope, acts as the product certification body.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Active cementitious coatings restore an alkaline, passivating environment and tolerate small application gaps, which suits most patch repairs. Barrier epoxy coatings isolate the steel completely but can create an anode next to any uncoated steel, so continuity of the coating matters. The repair design under EN 1504-9 determines the principle.

    A coating that protects the bar but reduces its bond to the repair mortar changes the structural behaviour of the member. EN 1504-7 therefore requires the pull-out bond of coated bars to be at least 80 % of that of uncoated bars, so the coating does not act as a bond breaker.

    Ribbed reinforcing bars of the agreed diameter, coated by the client or in the laboratory to the data sheet thickness, plus uncoated bars from the same lot as references, and sufficient product to coat them. Concrete for the pull-out specimens is cast in the laboratory.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing