    EAD 330083-02-0601 is the EOTA European Assessment Document for power-actuated fasteners for multiple use in concrete for non-structural applications. Amstelfy Technical Solutions tests powder- and gas-actuated nails and threaded studs against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): installation and functioning, characteristic resistance in concrete and durability. The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 330083-02-0601 covers nails and threaded studs that are driven into concrete by a powder-actuated or gas-actuated tool, without drilling, for multiple fixings of non-structural elements. The fastener is set by driving energy rather than by expansion or bond, so its resistance depends on penetration depth, base-material strength and the tool setting. The fastenings are also redundant: an element is held by several fasteners so that one failing fastener passes its load to its neighbours, which is why a single characteristic resistance valid for all load directions, together with conditions on the number of fixings and the load per fixing point, replaces the full set of failure-mode resistances used for structural anchors. Installation and functioning, resistance in cracked and uncracked concrete and durability of the hardened, usually zinc-plated steel are assessed. The current EOTA edition is version 04.

    Assessment programme

    Production fasteners are driven with the manufacturer's tool and cartridge or gas charge into concrete members covering the claimed strength range, at the specified penetration depth; series at the extremes of the driving-energy setting show how sensitive the fixing is to tool adjustment. Tension pull-out tests are run in uncracked and in cracked concrete, with the crack width prescribed by the EAD, and shear tests where required; a functioning series applies crack movement or repeated loading to installed fasteners. Durability is addressed through the coating specification and tests suited to hardened steel, and the use is normally limited to dry internal conditions unless corrosion-resistant steel is assessed.

    What the report states

    The report gives per fastener type, penetration depth and concrete strength the pull-out loads, failure modes (pull-out, spalling, shank failure), displacements and the 5 % fractile, plus the ratios from the driving-energy and functioning series. The TAB derives the characteristic resistance FRk, the admissible base materials and thicknesses, minimum spacing and edge distances, the fixing conditions for redundancy and the installation instructions for the ETA.

    Where the result is required

    Power-actuated fastenings under this EAD fix suspended ceilings, cable trays, conduit, pipe clips, insulation hangers, metal decking and formwork to concrete where speed of installation matters and the fixing is non-structural and redundant. The ETA provides the data for verification by the redundancy rules of the EAD, and the fastener is CE marked under the AVCP system stated in the EAD. Drilled fasteners for the same redundant systems are assessed under EAD 330747, and fasteners for single structural fixings under EAD 330232.

    What we assess

    • installation and functioning
    • characteristic resistance in concrete
    • durability

    Products covered

    • powder- and gas-actuated nails and threaded studs

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    It means the fastening is designed so that failure of one fastener does not cause collapse: the element is attached at several fixing points, the design load per fixing point is capped and the load redistributes to neighbouring fasteners. Because of this redundancy the EAD accepts a simplified test programme and a single characteristic resistance instead of the full structural anchor assessment.

    A driven fastener is set by the energy of the cartridge or gas charge and the piston of the tool, not by torque or bond. Penetration depth, spalling and pull-out resistance all change with the setting, so the ETA names the tool, the cartridge strengths or gas and the power setting, and series at reduced and increased energy prove that the fastening still functions at both ends of the range.

    Cracked concrete is covered once the tension series in cracked members and the crack-movement test have been passed, and most ETAs include it. Outdoor or damp use is usually excluded because hardened steel nails rely on a thin zinc coating; stainless or specially coated variants can be assessed for other exposure conditions if the manufacturer provides the durability evidence.