US qualification standard

    ASTM D5385 - Standard test method for hydrostatic pressure resistance of waterproofing membranes

    Testing · NAC-037-TL

    In short

    ASTM D5385 - Standard test method for hydrostatic pressure resistance of waterproofing membranes. Amstelfy's laboratory in Amstelveen performs this ASTM method for underground waterproofing membranes: hydrostatic pressure resistance. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ASTM D5385 determines

    ASTM D5385/D5385M determines the hydrostatic pressure resistance of waterproofing membranes intended for below-grade situations where water stands against the membrane under pressure. The membrane is applied to a substrate as it would be in service, sealed into a pressure cell and loaded with water on its exposed face; the pressure is raised in increments and held at each level so that leakage through the membrane, through a seam or along the bond to the substrate can develop. The highest pressure sustained without leakage is the result, usually expressed as a head of water and as pressure in kPa or psi. The method applies to sheet, self-adhered and liquid-applied membranes alike, which makes it the common yardstick of US below-grade waterproofing specifications, and it tests the membrane together with its bond, unlike the European sheet methods that test the unbonded sheet.

    Specimens, conditioning and procedure

    The client specifies the substrate and application: the membrane is applied to a concrete or mortar substrate at the thickness or with the adhesion method used on site, with a seam included where joint performance is claimed, and cured or conditioned for the period the product requires. The specimen is mounted in the hydrostatic pressure apparatus with the membrane face towards the water chamber and the substrate side open to observation. Water pressure is applied and increased in the increments and holding periods specified by the method, and the specimen is observed for water appearing on the back face or at the edge of the bond. The test ends at leakage or at the maximum pressure requested.

    What the report states

    The report states, for each specimen, the highest pressure held without leakage and the pressure at which leakage occurred, expressed in kPa or psi and as the equivalent head of water, the location and mode of leakage, the substrate, application thickness, curing and whether a seam was included. The manufacturer uses the value in product data and in the technical file for a US evaluation report; it is not a European declared characteristic.

    Where the result is required

    Specified for below-grade waterproofing in US project specifications and manufacturer data sheets, and part of ICC-ES evaluation programmes and other US acceptance criteria for waterproofing membranes under foundation walls and slabs, blind-side applications and tunnel linings. European manufacturers entering the US market test here before shipping samples, and the result is also read next to EN 1928 method B, which loads an unbonded sheet rather than the bonded system.

    What we assess

    • hydrostatic pressure resistance

    Products covered

    • underground waterproofing membranes

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    EN 1928 tests the sheet alone, clamped in a cell, and gives pass or fail at a pressure set by the product standard. ASTM D5385/D5385M tests the membrane applied to its substrate, so adhesion and seams are part of the result, and it raises the pressure in steps until leakage, giving a maximum head of water. The two are complementary, not interchangeable.

    The ones used in the field: for a self-adhered sheet a primed concrete surface, for a liquid-applied membrane the declared dry film thickness on concrete, for a pre-applied blind-side membrane the concrete cast against it. Including a seam or a detail answers the question most specifiers ask, because leakage in service usually starts at a seam or a termination rather than in the field of the membrane.

    As the highest pressure the membrane held without leakage, in kPa or psi, converted to the equivalent height of a water column, which is how below-grade specifications are written, for example a membrane rated for a given depth of water table. The report also gives the pressure and location at which leakage finally occurred, which distinguishes a membrane failure from a bond or seam failure.

    Related standards

    All Waterproofing membranes, roof underlays & liquid-applied systems testing