Test method

    EN 12390-8 - Testing hardened concrete - depth of penetration of water under pressure

    Testing · NAC-037-TL

    In short

    EN 12390-8 - Testing hardened concrete - depth of penetration of water under pressure. Amstelfy's laboratory determines water penetration depth of concrete according to EN 12390-8 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 12390-8 determines

    EN 12390-8 assesses the resistance of hardened concrete to water under pressure by measuring how far water penetrates into a specimen in a fixed time. Water at a pressure of 500 ± 50 kPa is applied to one face of a cube, cylinder or prism for 72 ± 2 h; the specimen is then split perpendicular to that face and the maximum depth reached by the water front is measured. The depth integrates the effect of water-cement ratio, compaction, curing and any waterproofing admixture or crystalline additive on the capillary pore structure. It is an index of impermeability rather than a permeability coefficient, and it is the quantity that national rules and project specifications for water-retaining and water-resisting concrete usually limit.

    Specimens, conditioning and procedure

    Specimens with a minimum dimension of 150 mm are made under EN 12390-2; the face that will receive the water is roughened with a wire brush immediately after demoulding so that the laitance layer does not seal it. Testing starts at an age of at least 28 days. The specimen is clamped in the pressure cell with the test face sealed around its perimeter and the opposite face exposed, and the pressure is held for the full duration while the other faces are inspected for water appearance. Afterwards the specimen is removed, wiped, split in half, and the water front is marked as soon as it is visible. One cell per specimen; sets of three are usual.

    What the report states

    The report gives the maximum penetration depth of each specimen in millimetres, the pressure and duration applied, the age at testing, the test face used relative to casting and a sketch or photograph of the water front. Where a specification sets a limit on the mean or the maximum depth, the report states the values for comparison.

    Where the result is required

    Impermeable and water-resisting concrete under national complements to EN 206, basement and tank concrete specifications, tunnel linings and precast elements, and the qualification of waterproofing admixtures, crystalline additives and repair concretes. It provides the hardened-concrete evidence that accompanies watertightness claims in product assessments and is often run on the same batch as EN 12390-3 cubes so strength and penetration are reported together.

    What we assess

    • water penetration depth

    Products covered

    • concrete

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Not the trowelled top face. The standard requires a moulded face, roughened with a wire brush straight after demoulding so that the cement skin does not act as a seal. The face is recorded in the report because results from different faces are not comparable.

    No. The depth after 72 h at 500 kPa is an index value that ranks concretes and checks compliance with a specified maximum. A coefficient of permeability needs a steady-state flow measurement under different conditions. Specifications written around EN 12390-8 quote depths in millimetres.

    Yes, by testing a reference concrete and the same concrete with the admixture side by side at the same age. The reduction in penetration depth is the comparative evidence; the client should state the dosage and the reference mix so the report documents both.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing