Test method

    EN 1848-2 - Flexible sheets for waterproofing - length, width, straightness and flatness - plastic and rubber sheets

    Testing · NAC-037-TL

    In short

    EN 1848-2 - Flexible sheets for waterproofing - length, width, straightness and flatness - plastic and rubber sheets. Amstelfy's laboratory determines length, width, straightness, flatness of plastic and rubber sheets according to EN 1848-2 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 1848-2 determines

    EN 1848-2 determines the length, width, straightness and flatness of plastic and rubber waterproofing sheets as delivered in rolls. Thermoplastic and elastomeric membranes are extruded or calendered thin and wound under tension, so they can show edges that wander and surfaces that are wavy or bulge when laid out, and a wavy sheet cannot be welded with a uniform seam or fixed flat under a mechanical fastener. The method unrolls the sheet, measures the length and the width at intervals, determines the straightness as the edge deviation from a stretched line and, in addition to the bitumen-sheet method, the flatness as the height of waves or bulges above the flat surface after the sheet has relaxed. All four are compared with the values the manufacturer declares and the tolerances in the product standard.

    Specimens, conditioning and procedure

    The roll is conditioned at the standard temperature and unrolled without tension on a flat surface, and the sheet is allowed to relax for the time the standard specifies. Length is measured along the sheet, width at several points, and straightness by the greatest distance between an edge and a line stretched along it over the reference length. For flatness the sheet is examined for waviness, bulges and folds and the maximum height above the surface is measured with a rule or gauge. Results are compared with the nominal values and the tolerances of the product standard, and the position of specimens for the remaining tests is marked on the relaxed sheet.

    What the report states

    The report gives the length in m, the width in mm as individual values and mean, the straightness deviation in mm over the reference length and the flatness as the maximum wave or bulge height in mm, with the declared nominal values and a statement of conformity with the tolerances of the product standard. The manufacturer declares length, width and straightness, and flatness where required, in the Declaration of Performance.

    Where the result is required

    Required by EN 13956 for plastic and rubber roofing sheets, EN 13967 for damp proof and tanking sheets, EN 13984 for vapour control layers and EN 13859-1 and EN 13859-2 for plastic underlays, as the opening step of type testing and as a factory production control check after winding. Installers rely on the declared width and straightness for seam planning with automatic welders. Bitumen sheets are measured by EN 1848-1.

    What we assess

    • length, width, straightness, flatness

    Products covered

    • plastic and rubber sheets

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Automatic hot-air and hot-wedge welders need both sheets flat against each other across the full seam width; a wave or bulge lifts one sheet and leaves a channel that water can follow. Flatness is therefore measured after the sheet has relaxed, and the product standard sets a limit so that a sheet can be seamed without stretching or cutting.

    Yes. Winding leaves a thermoplastic sheet curved and slightly stretched; measured immediately it can read shorter and wavier than it is. The standard specifies a relaxation time on the flat surface at the standard temperature before measurements are taken, and the report states the conditioning so that results from different laboratories are comparable.

    EN 1848-1 for bitumen sheets measures length, width and straightness only; the stiff carrier of a bitumen sheet keeps it flat. Part 2 adds flatness and a relaxation period because thin plastic and rubber sheets behave differently after unwinding. Both parts otherwise unroll the whole sheet and compare the measurements with declared values and tolerances.