Test method

    EN 14651 – Fibre reinforced concrete flexural test

    Test method for metallic fibre concrete - flexural tensile strength (LOP, residual)

    Testing · NAC-037-TL

    In short

    EN 14651 - Test method for metallic fibre concrete - flexural tensile strength (LOP, residual). Amstelfy's laboratory determines limit of proportionality and residual flexural strengths fR1-fR4 of steel fibre reinforced concrete according to EN 14651 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 14651 determines

    EN 14651 is the reference method for the flexural tensile behaviour of metallic fibre concrete and, by extension through EN 14889-2, of macro polymer fibre concrete. A beam with a sawn notch at mid-span is loaded in three-point bending while the crack mouth opening displacement, CMOD, is measured across the notch and used to control the test. From the load–CMOD curve the limit of proportionality fL is calculated from the highest load in the interval up to 0.05 mm, and residual flexural tensile strengths fR,1, fR,2, fR,3 and fR,4 are calculated at CMOD values of 0.5, 1.5, 2.5 and 3.5 mm. These residual strengths are the input for structural design with fibre concrete in fib Model Code 2010 and national annexes, and the basis of the fibre performance classes.

    Specimens, conditioning and procedure

    Beams of 150 × 150 mm cross-section and 550 to 700 mm length are cast in the manner the standard prescribes, cured, then rotated 90° about their longitudinal axis and notched at mid-span to a remaining depth of 125 mm with a notch not wider than 5 mm. The beam is placed on roller supports 500 mm apart and loaded through a central roller. A clip gauge across the notch measures CMOD; the machine is run in closed-loop CMOD control at 0.05 mm/min until 0.1 mm and 0.2 mm/min thereafter, to a CMOD of at least 4 mm. Deflection control is permitted using the conversion given in the standard. Fibre count on the fracture surface may be requested.

    What the report states

    The report gives fL and fR,1 to fR,4 in MPa for each beam, computed from the load, span and the notched section, the complete load–CMOD curves, beam dimensions, age, fibre type and dosage, and the mean of the set. For a fibre product the client derives the characteristic values needed for the EN 14889 declaration or for a performance class.

    Where the result is required

    The effect-on-concrete-strength declaration for structural fibres under EN 14889-1 and EN 14889-2 via EN 14845-2, design of fibre-reinforced slabs, tunnel segments, shotcrete linings and precast elements to fib Model Code 2010 and national rules, and the fibre classification in EN 1992 developments. It is also the European side of dual programmes that include ASTM C1609 for the US market.

    What we assess

    • limit of proportionality and residual flexural strengths fR1-fR4

    Products covered

    • steel fibre reinforced concrete

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The notch fixes the crack location so that CMOD can be measured and controlled at a known section. Rotating the beam puts a moulded side face in tension rather than the trowelled top, removing the surface effects of finishing and fibre settlement from the result.

    EN 14651 reports individual beams; the number is set by the referencing document. EN 14845-2 programmes and performance classification use sets large enough to derive characteristic values, and a minimum of six per dosage is common, often twelve where the scatter of macro fibres is expected to be high.

    No. The two methods differ in loading arrangement, notch, control variable and the points at which residual strength is read. Where both markets are targeted, both tests are run from the same batches; the results are reported separately and not converted.

    Related standards

    All Concrete, fibres, mortars & concrete repair products testing