Test method

    EN 12311-2 - Flexible sheets for waterproofing - tensile properties - plastic and rubber sheets

    Testing · NAC-037-TL

    In short

    EN 12311-2 - Flexible sheets for waterproofing - tensile properties - plastic and rubber sheets. Amstelfy's laboratory determines tensile strength and elongation of plastic and rubber sheets according to EN 12311-2 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 12311-2 determines

    EN 12311-2 determines the tensile properties of plastic and rubber waterproofing sheets and provides two methods because these products fall into two mechanically different groups. Method A uses strips of 50 mm width and reports the maximum force per 50 mm and the elongation at maximum force; it suits sheets with a fabric or fleece reinforcement, whose strength is governed by the scrim rather than by the polymer. Method B uses dumbbell specimens cut with a die and reports tensile strength as a stress in N/mm² and elongation at break; it suits homogeneous, unreinforced sheets, whose polymer matrix carries the load. In both cases the specimen is stretched at a constant speed until rupture in both roll directions, and the result characterises the response of the membrane to substrate movement, wind suction and installation stresses.

    Specimens, conditioning and procedure

    Specimens are cut in the longitudinal and transverse direction away from the roll edges and conditioned in the standard laboratory climate. For method A, strips 50 mm wide are clamped at the initial grip separation given in the standard and pulled at the speed the method prescribes until rupture, recording force and extension. For method B, dumbbell specimens are punched from the sheet, their thickness is measured in the narrow section, reference marks define the gauge length and the specimen is pulled at the speed the method prescribes while extension between the marks is followed. Maximum force or strength and the corresponding elongation are read from each curve. Means per direction are calculated and the failure appearance is noted.

    What the report states

    For method A the report gives the maximum tensile force in N per 50 mm and the elongation at maximum force in per cent; for method B the tensile strength in N/mm² and the elongation at break in per cent, each per direction as means with individual values and the measured thickness. The manufacturer declares the values with the tolerance the product standard allows, and after ageing the retained percentages are reported.

    Where the result is required

    Cited by EN 13956 for plastic and rubber roofing sheets, EN 13967 for damp proofing and tanking sheets, EN 13984 for plastic vapour control layers and EN 13859-1 and EN 13859-2 for plastic underlays, with the method chosen according to whether the sheet is reinforced. The elongation from method B is also the basis for judging unreinforced membranes on moving substrates, and the force from method A feeds wind-load design of mechanically fixed roofs. Bitumen sheets use EN 12311-1.

    What we assess

    • tensile strength and elongation

    Products covered

    • plastic and rubber sheets

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Reinforced sheets, those with a polyester scrim, glass fleece or fabric, are tested by method A because the reinforcement governs the force. Homogeneous sheets without reinforcement use method B, where stress and elongation at break describe the polymer. The product standard names the method for each product type, and the report states which one was used.

    Method A reports elongation at maximum force, which for a reinforced sheet is the strain at which the scrim breaks, often well below 50 per cent. Method B reports elongation at break of a homogeneous polymer, which for EPDM or plasticised PVC can exceed several hundred per cent. The two numbers describe different things and are not compared.

    No. EN ISO 527-3 is the general plastics film method with its own specimen geometry and speeds; EN 12311-2 is the method the waterproofing product standards cite, with 50 mm strips for reinforced sheets and specific dumbbells for homogeneous ones. Data from EN ISO 527-3 is useful for material development but cannot be entered in a Declaration of Performance under EN 13956 or EN 13967.

    Related standards

    All Waterproofing membranes, roof underlays & liquid-applied systems testing