European Assessment Document

    EAD 340351-00-0104 - Fibre reinforced polymer kits made of a pultruded carbon fibre laminate and an epoxy adhesive

    Testing · NAC-037-TLCertification · NAC-026-PPSETA route

    In short

    EAD 340351-00-0104 is the EOTA European Assessment Document for fibre reinforced polymer kits made of a pultruded carbon fibre laminate and an epoxy adhesive. Amstelfy Technical Solutions tests CFRP laminate strengthening kits against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): tensile properties of laminate, adhesive and bond properties, durability (temperature, moisture, alkalinity, UV) and creep. The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 340351-00-0104 covers kits in which a factory-made pultruded carbon fibre laminate is bonded to concrete with a two-component epoxy adhesive to increase the flexural or tensile capacity of a member. Because the laminate leaves the plant fully cured, its tensile strength, modulus and ultimate strain can be characterised as a product property, and the uncertainty of the system lies in the adhesive joint: its strength, its glass transition temperature and how both evolve with heat, moisture, alkalinity and sustained stress. The EAD therefore separates the assessment into laminate properties, adhesive properties, bond between laminate and concrete, and durability of each. The resulting ETA lists the values a designer needs for CNR-DT 200 or fib Bulletin 90 style calculations, including the anchorage length and the limiting bond stress.

    Assessment programme

    Laminate coupons are cut from production strips of each thickness and width family and tested in tension with bonded tabs; the modulus is measured with extensometers or strain gauges in the longitudinal fibre direction. The adhesive is characterised on cast specimens for tensile and shear strength, modulus, and glass transition temperature after the curing schedule given by the manufacturer. Bond is tested by pull-off from a concrete substrate and by shear tests in which a bonded laminate is pulled from a concrete prism, recording load against slip. Durability series repeat these tests after exposure to elevated temperature, humidity, alkaline solution, freeze-thaw and, for the laminate, UV radiation, and the bond is held under sustained load to measure creep.

    What the report states

    The report states laminate tensile strength, modulus and strain at failure as mean and characteristic values per laminate type; adhesive strengths and glass transition temperature; pull-off strength with failure location; shear-bond capacity and the slip at which debonding started; and creep deformation over time. Retained properties after each ageing condition are expressed relative to the reference series. These are the quantities the TAB transfers into the ETA performance tables.

    Where the result is required

    Bonded CFRP plates are the standard retrofit for under-reinforced beams and slabs, for bridge decks with widened lanes, and for members with corroded reinforcement. The ETA supports the design of plate width, anchorage length and end detailing. Manufacturers who also sell wet lay-up fabrics usually run the sister programme under EAD 340352, and specifiers compare laminate ETAs on modulus class and declared bond stress. Tests reference the plastics methods of the EN ISO 527 series for the laminate and the pull-off method of EN 1542 for bond.

    What we assess

    • tensile properties of laminate
    • adhesive and bond properties
    • durability (temperature, moisture, alkalinity, UV)
    • creep

    Products covered

    • CFRP laminate strengthening kits

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    Several metres of each laminate type to be declared, ideally from more than one production run, plus enough adhesive to cast the adhesive specimens and bond the shear and pull-off assemblies. Concrete test blocks are usually prepared in the laboratory to a defined strength class so that bond results are comparable between manufacturers.

    Above the glass transition temperature of the adhesive the joint softens and the plate can no longer transfer its force into the concrete. The ETA uses the measured value to set the maximum service temperature of the system, so a low value restricts use on sun-exposed decks or near heat sources even if the laminate itself is unaffected.

    Yes. Pultruded carbon strips fail at the grips without protection, which gives low and scattered results. Tabs of glass fibre composite or aluminium are bonded to both ends, and the test is only valid when rupture occurs in the free length. The strain is measured away from the tabs over a defined gauge length.