European Assessment Document

    EAD 260001-00-0303 - Structural sections made from fibre reinforced polymers (FRP / glass fibre composites)

    Testing · NAC-037-TLCertification · NAC-026-PPSETA route

    In short

    EAD 260001-00-0303 is the EOTA European Assessment Document for structural sections made from fibre reinforced polymers (frp / glass fibre composites). Amstelfy Technical Solutions tests pultruded FRP profiles against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): tensile, compressive, flexural and shear properties, pin-bearing strength, durability and creep and glass transition temperature. The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 260001-00-0303 covers structural sections made by pultrusion from glass or other fibres in a thermoset resin: I, channel, angle, tube, plate and purpose-made shapes used as beams, columns, bracing, gratings and bridge-deck elements. Because the material is orthotropic and the wall thickness is thin relative to the section, the assessment characterises mechanical properties in the longitudinal and transverse directions of the laminate, adds full-section stiffness and strength where the ETA is to cover member behaviour, and establishes connection-relevant properties such as pin-bearing strength for bolted joints. Durability and creep are central because glass fibre composites lose stiffness under sustained load and strength under moisture, heat and alkaline exposure. The ETA values are the inputs for design to CEN/TS 19101 or to the manufacturer-specific approaches used in national practice.

    Assessment programme

    Coupons are cut from the flanges and webs of production sections and tested for tension in both directions to EN ISO 527-4, compression, flexure to EN ISO 14125, in-plane and interlaminar shear, and pin-bearing strength with a bolt through a drilled hole. Fibre content, density, glass transition temperature by DMA or DSC and water absorption complete the material characterisation. Full sections may be tested in three- or four-point bending to obtain the effective flexural and shear moduli, and in compression where column behaviour is claimed. Durability series condition coupons in water, alkaline solution, heat and UV before re-testing; creep tests hold coupons or sections under sustained load and record deformation over the period required for extrapolation.

    What the report states

    Reported per section family and per direction: tensile and compressive strength and modulus, flexural strength and modulus, shear strengths, pin-bearing strength per bolt diameter and edge distance, glass transition temperature, fibre content and density, with characteristic values where the EAD requires them. Full-section tests yield effective moduli for deflection calculation. Retained properties after conditioning and creep coefficients for the declared time periods are tabulated for the ETA.

    Where the result is required

    Pultruded profiles are used where corrosion, weight or electromagnetic transparency rule out steel: footbridges, cooling-tower structures, platforms and walkways in chemical and offshore plants, rail trackside structures, and secondary structures in buildings. An ETA under this EAD supports CE marking of profiles as structural products; EN 13706 remains the reference for the E17 and E23 grade system that many specifications still cite, and the same coupon methods serve both routes. Grids and bars from the same producers are assessed under EAD 340392 and EAD 260023.

    What we assess

    • tensile, compressive, flexural and shear properties
    • pin-bearing strength
    • durability and creep
    • glass transition temperature

    Products covered

    • pultruded FRP profiles

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    From each distinct element of the profile, flange and web, in both the pultrusion direction and across it, because the fibre architecture and the roving-to-mat ratio differ between elements. The cutting plan is recorded and the ETA may declare separate values for flanges and webs when they differ.

    It is the stress at which the laminate crushes or splits in front of a bolt, and it governs bolted connection capacity in pultruded structures. The test loads a pin through a hole in a coupon with defined edge and end distances; results depend on these distances and on the bolt diameter, so the ETA states the geometry tested.

    Coupon data describe the laminate; the EAD allows and manufacturers normally request full-section bending tests because shear deformation of thin webs makes the effective member stiffness lower than the coupon modulus suggests. Section tests also reveal local buckling and web crippling, which coupon tests cannot show.

    Related standards

    All FRP, FRCM/CRM strengthening & FRP reinforcement testing