Test method

    EN ISO 527 - Plastics - determination of tensile properties

    Testing · NAC-037-TL

    In short

    EN ISO 527 - Plastics - determination of tensile properties. Amstelfy's laboratory determines tensile properties of plastics according to EN ISO 527 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 527 determines

    EN ISO 527 is the multi-part standard for determining tensile properties of plastics. Part 1 contains the principles, definitions and reporting rules; part 2 covers moulding and extrusion plastics with injection-moulded or machined dumbbells; part 3 covers films and sheets; part 4 isotropic and orthotropic fibre-reinforced composites; part 5 unidirectional composites. All parts share one physical test: a specimen of defined geometry is extended at constant speed and the stress on the original cross-section is plotted against strain. What changes between parts is the specimen shape, the need for tabs, the speeds and the strain measurement. Quoting the series number alone therefore does not define a test; a report must name the part, specimen type, speed and conditioning, and this page helps select them.

    Specimens, conditioning and procedure

    The part is chosen by material: moulded or extruded thermoplastics and thermosets go to part 2, films below 1 mm to part 3, laminates with fabrics, mats or short fibres to part 4, unidirectional laminates to part 5. Specimens are moulded, punched or machined accordingly, measured and conditioned in the standard atmosphere, and tested with a minimum of five per direction. The modulus is measured with an extensometer between 0.05 % and 0.25 % strain, then the test runs to failure at the specified speed. The laboratory records specimen type, speed, extensometer type and failure location, which are the details that make results between manufacturers and between batches comparable.

    What the report states

    The report identifies the part and specimen type, then lists tensile modulus, stress at yield, tensile strength, strain at yield and at break, and nominal strain at break where applicable, with means, standard deviations and individual values, and curves. For orthotropic materials results are per direction. Where a product specification sets requirements, the report states conformity against the declared or required values.

    Where the result is required

    Tensile properties according to the series are declared on nearly every plastics data sheet and required in product standards for pipes, profiles, sheets and geosynthetics, in EAD programmes for FRP strengthening kits, bars and profiles, and in ETICS and roofing kit assessments for plastic components. Retained tensile strength after heat, UV or chemical ageing is the standard indicator of durability in those documents, so the tensile test is usually run before and after conditioning.

    What we assess

    • tensile properties

    Products covered

    • plastics

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Short-fibre reinforced moulding compounds are tested to part 2 with injection-moulded dumbbells when the material is being qualified as a moulding compound, and to part 4 type 1B when it is treated as a composite with properties depending on flow orientation. The two give comparable results on similar specimens; the specification decides.

    No. Each part fixes specimens and tabs for a material class; a unidirectional carbon laminate tested as a part-4 strip breaks at the grips and underestimates strength. Conversely, a part-5 specimen is unnecessary for a woven fabric laminate. The part named in the report is part of the result's identity.

    At least five per direction and condition, conditioned in the standard atmosphere of ISO 291 unless the product standard requires another state such as dry-as-moulded or after immersion. Extra specimens are advisable for brittle composites where grip failures are likely to invalidate some tests.

    Related standards

    All Plastics, composites & metals - material test methods testing