European Assessment Document

    EAD 260023-00-0301 - Carbon, glass, basalt and aramid fibre reinforced polymer bars as reinforcement of structural elements

    Testing · NAC-037-TLCertification · NAC-026-PPSETA route

    In short

    EAD 260023-00-0301 is the EOTA European Assessment Document for carbon, glass, basalt and aramid fibre reinforced polymer bars as reinforcement of structural elements. Amstelfy Technical Solutions tests GFRP, CFRP, BFRP and AFRP rebars against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): tensile strength and modulus, bond to concrete, transverse shear and alkali resistance and durability. The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 260023-00-0301 covers FRP bars used in place of or alongside steel reinforcement in concrete elements. The bar is a unidirectional composite that is linear-elastic to failure, so the assessment cannot borrow the yield-based logic of reinforcing steel: it establishes the characteristic tensile strength and modulus, the bond behaviour of the surface finish, and the reduction of tensile capacity under sustained load, cyclic load and the alkaline pore solution of concrete. Further characteristics include transverse shear, cross-sectional area by immersion, glass transition temperature, fibre content, thermal expansion and the strength of bends. The ETA states these per bar type and diameter so that designers using fib Bulletin 40, the FRP annex of the new Eurocode 2 or national rules can derive design strengths with the environmental and long-term reduction factors.

    Assessment programme

    Bars of each diameter are received in straight lengths; the cross-section is measured by water displacement. Tensile tests use steel-tube anchors filled with expansive grout or resin so that failure occurs in the free length. Bond is measured by pull-out of a bar embedded over a short length in a concrete cube, recording the free- and loaded-end slip. Transverse shear uses a double-shear fixture. Alkali resistance immerses bars in a simulated pore solution at elevated temperature with and without tensile load before residual tensile tests. Creep rupture tests hold bars at several stress levels until failure, and fatigue tests apply the stress ranges given in the EAD. Bent bars are tested for the capacity of the bend.

    What the report states

    The report gives, per diameter, the nominal and measured area, mean and characteristic tensile strength and modulus, ultimate strain, bond strength and bond-slip curve, transverse shear strength, residual tensile strength after alkaline exposure, the creep-rupture regression with the extrapolated stress limit at the required lifetime, fatigue results, glass transition temperature and bend capacity. Characteristic values follow the statistical rule of the EAD, and the failure modes are recorded.

    Where the result is required

    FRP bars are specified for marine and coastal structures, bridge decks exposed to de-icing salts, tunnel soft-eyes where boring machines cut through the reinforcement, MRI rooms and other magnetically sensitive areas, and precast elements with thin cover. The ETA is the European route to a Declaration of Performance; in North America the same bars are specified under ASTM D7957 and designed under ACI 440.11. Component methods overlap with ISO 10406-1, and the GFRP rebar harmonisation work of the European Rebar Council draws on the same test set.

    What we assess

    • tensile strength and modulus
    • bond to concrete
    • transverse shear
    • alkali resistance and durability
    • creep rupture and fatigue

    Products covered

    • GFRP, CFRP, BFRP and AFRP rebars

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    Enough straight lengths for the tensile, bond, shear, alkali, creep and fatigue series, allowing for anchorage lengths of several hundred millimetres at each end of tensile specimens. Creep-rupture and fatigue consume the largest numbers because several stress levels are needed. Bent bars are supplied ready-formed from production, not bent in the laboratory.

    Glass and basalt fibres lose strength under sustained stress through stress corrosion, so the stress that can be held for the design life must be extrapolated from failures at higher stresses held for weeks to months. The programme runs several load levels in parallel, and the extrapolation method of the EAD fixes how far the data may be projected.

    The pull-out test ranks surface finishes and gives the characteristic bond strength used in the ETA. Anchorage and lap lengths are derived from it by the design code, sometimes with additional beam-type bond tests when the manufacturer wants to declare values for larger diameters or confined conditions.

    Related standards

    All FRP, FRCM/CRM strengthening & FRP reinforcement testing