US qualification standard

    ICC-ES AC320 - Acceptance criteria for fiber-reinforced polymer composite or unreinforced polymer connectors anchored in concrete

    Testing · NAC-037-TL

    In short

    ICC-ES AC320 - Acceptance criteria for fiber-reinforced polymer composite or unreinforced polymer connectors anchored in concrete. Amstelfy's laboratory in Amstelveen performs this US qualification protocol for FRP and polymer connectors for sandwich panels: tension and shear capacity, durability and creep. Testing is on the ISO/IEC 17025 accreditation scope NAC-037-TL, which lets European manufacturers prepare US evaluation-report programmes without shipping samples overseas.

    What ICC-ES AC320 determines

    ICC-ES AC320 sets out how fibre-reinforced polymer composite or unreinforced polymer connectors anchored in concrete are qualified for an ICC-ES evaluation report. The connectors tie the two concrete wythes of an insulated sandwich wall or a precast panel through the insulation layer and transfer the loads that result from wind, handling, thermal bowing and self-weight of the outer wythe. The criteria define the test programme that supports allowable or design loads in tension and shear for each connector type, embedment and insulation thickness, and require evidence that the polymer keeps those loads over time: sustained-load creep, exposure to the alkaline concrete environment, moisture, temperature and freeze-thaw. An evaluation report issued by ICC-ES on this basis allows the connector to be used in buildings designed under the International Building Code and ACI 318.

    Specimens, conditioning and procedure

    Connectors are cast into concrete test members that reproduce the panel build-up: inner wythe, insulation of the thickness to be recognised, outer wythe. Tension tests pull the outer wythe away from the inner one; shear tests load the assembly parallel to the panel plane, typically as symmetric double-shear specimens. Series are repeated for the concrete strengths, insulation thicknesses and connector embedments claimed. Creep specimens are held under a sustained fraction of the ultimate load while displacement is logged over the period set in the criteria. Durability series expose connectors or embedded assemblies to alkaline solution, elevated temperature, moisture and freeze-thaw cycling before residual-strength testing. Material tests on the polymer, including glass transition temperature, complete the file.

    What the report states

    Ultimate loads in tension and shear are reported per connector and per configuration with the coefficient of variation and the failure mode: polymer rupture, pull-out from the wythe, or concrete break-out. Creep curves are extrapolated to the service life required by the criteria and compared with the acceptance limits. Residual strengths after conditioning are given as ratios to the unconditioned reference. The report is formatted for submission to ICC-ES, which derives the allowable loads published in the evaluation report.

    Where the result is required

    Precast and tilt-up producers in North America use AC320 data to place connectors in insulated wall panels designed under IBC and ACI 318 without project-specific testing. European manufacturers of GFRP or polymer connectors who already hold or seek an ETA under EAD 330387 often run the AC320 series on the same product so that one development programme serves both markets. The two documents overlap in tension and shear testing but differ in conditioning regimes, statistical evaluation and the format of the published values.

    What we assess

    • tension and shear capacity
    • durability
    • creep

    Products covered

    • FRP and polymer connectors for sandwich panels

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    US and international evaluation-report programmes (ICC-ES, IAPMO UES, ACI 318 qualification) accept data from ISO/IEC 17025-accredited laboratories. Amstelfy runs these programmes in the Netherlands so European manufacturers avoid shipping samples overseas; the evaluation report itself is issued by the evaluation service.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Each thickness that the evaluation report is to list, because shear capacity and stiffness change with the free length of the connector between the wythes. Manufacturers usually bracket the range with the thinnest and thickest insulation and add intermediate points where interpolation is to be claimed. The concrete strength of each wythe is recorded for every series.

    Both load the connector in tension and shear through the insulation, but AC320 follows the ICC-ES evaluation framework with its own conditioning sequence, creep assessment and derivation of allowable loads, while the EAD leads to characteristic values in an ETA. Specimens can often be cast in one campaign, with the evaluation done separately for each document.

    The criteria are built around component specimens, which give statistically usable results per connector. Full-size panel tests are sometimes added by manufacturers to demonstrate composite action or thermal bowing behaviour, but they supplement rather than replace the component series that the evaluation report relies on.

    Related standards