Test method

    EN ISO 527-4 – Composite tensile test

    Plastics - tensile properties - isotropic and orthotropic fibre-reinforced composites

    Testing · NAC-037-TL

    In short

    EN ISO 527-4 - Plastics - tensile properties - isotropic and orthotropic fibre-reinforced composites. Amstelfy's laboratory determines tensile strength, modulus and strain of FRP laminates and composite coupons according to EN ISO 527-4 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 527-4 determines

    EN ISO 527-4 adapts the general tensile method of EN ISO 527-1 to fibre-reinforced plastic composites that are isotropic or orthotropic: short-fibre moulding compounds, mat and fabric laminates, and multidirectional lay-ups. Unidirectional laminates are excluded and go to EN ISO 527-5. A flat specimen is pulled at constant crosshead speed while force and strain are recorded; the tensile strength, the modulus between 0.05 % and 0.25 % strain, and the strain at failure follow from the cross-section and the extensometer signal. Because orthotropic laminates differ in the warp and weft or 0° and 90° directions, specimens are cut and reported per direction. The result is a material property of the laminate as manufactured, which feeds laminate design, ETA programmes and factory production control.

    Specimens, conditioning and procedure

    Three specimen types are defined: type 1B, a dumbbell for isotropic materials such as short-fibre compounds; type 2, a parallel-sided strip 25 mm wide (50 mm for coarse fabrics) without tabs; and type 3, the same strip with bonded end tabs for materials that would otherwise fail in the grips. Specimens are machined from plates or products with edges finished to avoid delamination, conditioned in the standard atmosphere, and tested with a minimum of five per direction. Strain is measured over a 50 mm gauge length by contact or optical extensometer or by strain gauges; crosshead displacement alone is not accepted for modulus. Test speed, specimen thickness and failure location are recorded, and tests failing at the grips are discarded.

    What the report states

    Per direction the report gives tensile strength in MPa, tensile modulus in GPa, strain at tensile strength and at break in %, and where measured Poisson's ratio, each as mean, standard deviation and coefficient of variation with individual values. Specimen type, dimensions, conditioning and test speed are stated, together with the failure mode and location. Characteristic values are added when a product assessment requires them.

    Where the result is required

    The method underpins the laminate values in ETAs for FRP fabric kits under EAD 340352, pultruded profiles under EAD 260001 and FRP grids, and is the usual tensile reference in EN 13706 for pultruded profiles and in composite product specifications for tanks, pipes and panels. Laminators use it for batch release and for qualifying new resin-fibre combinations. For bars and unidirectional strips the dedicated methods of EN ISO 527-5 or ISO 10406-1 are used instead.

    What we assess

    • tensile strength, modulus and strain

    Products covered

    • FRP laminates
    • composite coupons

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    When a type 2 strip fails at or inside the grips, which is common for high-strength woven carbon laminates and thin glass laminates. Tabs of cross-ply glass composite or aluminium spread the clamping pressure. The standard leaves the choice to the operator; the report states the type used so results can be compared.

    Flat regions of the product are identified and strips are machined with a diamond or carbide saw, then edge-finished, keeping track of the fibre direction. Curved or ribbed areas cannot be tested with this method; thickness variation along the gauge length is measured and limited before testing.

    Part 5 covers unidirectional laminates where nearly all fibres run one way; it uses its own specimen types with mandatory tabs and tests in the 0° and 90° directions. Part 4 covers everything else from short-fibre compounds to balanced fabrics. Using part 4 on a unidirectional laminate underestimates its strength because the strip fails at the grips.

    Related standards

    All Plastics, composites & metals - material test methods testing