Test method

    EN ISO 14125 – FRP flexural test

    Fibre-reinforced plastic composites - flexural properties

    Testing · NAC-037-TL

    In short

    EN ISO 14125 - Fibre-reinforced plastic composites - flexural properties. Amstelfy's laboratory determines flexural strength and modulus (3- and 4-point) of FRP laminates according to EN ISO 14125 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 14125 determines

    EN ISO 14125 determines the flexural properties of fibre-reinforced plastics by loading a beam specimen resting on two supports either at mid-span (method A, three-point) or at two points (method B, four-point) until it fails or reaches a limiting deflection. Flexural stress is calculated from outer-fibre bending theory, flexural strain from the mid-span deflection, and the modulus from the slope between two defined strains. Because a short beam fails in interlaminar shear rather than in bending, the standard assigns a span-to-thickness ratio to four material classes, from short-fibre thermoplastics to unidirectional laminates, with the longest spans for the stiffest, most shear-sensitive laminates. The result characterises the laminate as a beam, which is how pultruded profiles, panels and strengthening plates are often loaded in service.

    Specimens, conditioning and procedure

    Rectangular specimens are cut from plates or products in the fibre direction of interest, with length, width and span chosen from the class table of the standard for the measured thickness. After conditioning in the standard atmosphere, at least five specimens per direction are loaded at a constant crosshead speed on cylindrical supports and loading noses of the specified radii. Deflection is measured at mid-span with a transducer, not from crosshead travel, when modulus is required. Method A is the default; method B is chosen when the material is prone to local crushing under a single nose or when a region of constant bending moment is wanted, for instance for unidirectional carbon laminates.

    What the report states

    The report gives flexural strength in MPa, flexural modulus in GPa, strain at break or at the stress maximum, the span-to-thickness ratio and method used, and the failure mode: tensile fibre failure on the bottom face, compression or buckling on the top face, or interlaminar shear, which invalidates the result as a flexural value. Means, standard deviations and individual values are listed per direction.

    Where the result is required

    Flexural data are required in ETAs for pultruded sections under EAD 260001, in EN 13706 for profile grading, and in specifications for composite panels, gratings, cladding and boat and vehicle laminates. Manufacturers use the test for incoming-material and batch control because it needs small specimens and reacts to cure quality and fibre wet-out. For unreinforced or short-fibre moulded plastics the simpler EN ISO 178 applies, and for sandwich panels a different method is used.

    What we assess

    • flexural strength and modulus (3- and 4-point)

    Products covered

    • FRP laminates

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Three-point loading (method A) is the default and suits most mat and fabric laminates. Four-point loading (method B) is preferred for unidirectional and high-modulus laminates where a single loading nose would crush the surface, and when the client's specification or an EAD programme names it. Results from the two methods are not directly comparable.

    A composite beam carries bending stress in the fibres and shear in the resin between plies. If the span is short relative to the thickness, the shear stress reaches the interlaminar strength first and the specimen delaminates instead of breaking in bending. Longer spans for stiffer laminates keep the failure in bending.

    No. The flexural modulus combines tensile and compressive behaviour of the outer plies and is affected by shear deformation and the lay-up sequence, so it usually differs from the EN ISO 527-4 tensile modulus. Design codes specify which is needed; both are often determined on the same laminate.

    Related standards

    All Plastics, composites & metals - material test methods testing