Test method

    EN ISO 604 - Plastics - compressive properties

    Testing · NAC-037-TL

    In short

    EN ISO 604 - Plastics - compressive properties. Amstelfy's laboratory determines compressive strength and modulus of plastics and composites according to EN ISO 604 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 604 determines

    EN ISO 604 determines the compressive properties of plastics: a prismatic or cylindrical specimen is compressed between parallel platens at constant speed until it yields, fractures or reaches a set strain, and the stress on the original cross-section is plotted against the compressive strain. Compression of a slender specimen is complicated by buckling, so the standard uses two specimen geometries: a short specimen for compressive strength and yield stress, and a longer specimen with a controlled slenderness ratio for the modulus, measured with an extensometer or strain gauges between 0.05 % and 0.25 % strain. The result describes the material under compressive loading, which matters for struts, bearing pads, thick-walled mouldings and for composites, whose compressive strength is often below the tensile strength because of fibre micro-buckling.

    Specimens, conditioning and procedure

    Specimens are machined or moulded with end faces flat, parallel and perpendicular to the axis; the preferred strength specimen is 10 mm long and the modulus specimen 50 mm long, both 10 mm wide and 4 mm thick, with other sizes permitted provided the slenderness limits of the standard are kept. After conditioning, at least five specimens per property are loaded between hardened platens, one of them self-aligning, at the speed assigned to the property. Strain for the modulus is taken from an extensometer mounted on the specimen or from strain gauges on opposite faces to detect bending. Specimens that buckle or fail at the end faces are reported as such and replaced.

    What the report states

    The report gives compressive strength and compressive yield stress in MPa, strain at yield or at break in %, and compressive modulus in MPa from the long specimen, each with mean and standard deviation, plus specimen type, dimensions, slenderness ratio, test speed and the failure appearance: shear fracture, crushing, splitting or buckling. For composites, the loading direction relative to the fibres is stated.

    Where the result is required

    Compressive data are requested in ETAs for pultruded profiles under EAD 260001, where column and web crippling checks need the compressive strength of the laminate, in specifications for load-bearing thermoplastic parts, spacers and insulation support blocks, and in material qualifications for polymer concrete and grouts cast in test moulds. Thick composite laminates may instead be tested with composite-specific fixtures; EN ISO 604 remains the common method for unreinforced plastics and short-fibre compounds.

    What we assess

    • compressive strength and modulus

    Products covered

    • plastics
    • composites

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    A short block resists buckling and gives the true compressive strength, but its ends restrain lateral expansion so the strain field is not uniform enough for modulus. A longer specimen gives a clean strain measurement but must stay below the slenderness ratio at which it buckles elastically. The standard therefore prescribes both.

    Yes, if a flat region thick enough for the slenderness requirements exists and the end faces can be machined flat and square. Thin walls can be tested as shorter specimens for strength only. The cutting direction relative to flow or fibre orientation is recorded because it changes the result.

    Shear fracture through the specimen, crushing or splitting parallel to the load are valid. Buckling, visible as a lateral bow before the maximum force, and crushing confined to a damaged end face invalidate the specimen, which is reported and replaced from the spare specimens.

    Related standards

    All Plastics, composites & metals - material test methods testing