Test method

    EN 12664 – Thermal conductivity testing

    Thermal performance of building materials - guarded hot plate and heat flow meter - dry and moist products of medium and low thermal resistance

    Testing · NAC-037-TL

    In short

    EN 12664 - Thermal performance of building materials - guarded hot plate and heat flow meter - dry and moist products of medium and low thermal resistance. Amstelfy's laboratory determines thermal resistance (medium/low resistance) of thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre) and building materials according to EN 12664 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 12664 determines

    EN 12664 covers materials whose thermal resistance is too low for EN 12667: dense or thin products such as concrete, mortar, masonry material, gypsum, wood-based panels, plastics and rubber, in dry or moist condition. The measurement uses the same guarded hot plate or heat flow meter apparatus, but two problems dominate at low resistance. First, the thermal contact resistance between the plates and a rigid specimen becomes a significant part of the total, so the standard requires measures such as contact sheets or surface temperature sensors. Second, a temperature gradient drives moisture through a moist specimen and changes what is being measured, so moist specimens are tested sealed and quickly, with moisture content determined before and after. The result is the thermal resistance at the stated mean temperature and moisture state, from which conductivity follows for homogeneous specimens.

    Specimens, conditioning and procedure

    Specimens are slabs with flat, parallel faces, machined where necessary, sized to the apparatus plates and thick enough to give a measurable resistance. Dry specimens are dried to constant mass by the procedure appropriate to the material; moist specimens are conditioned to the intended moisture content, weighed, sealed in a vapour-tight envelope and weighed again after the test. Surface temperatures are measured with sensors on the specimen faces or the contact resistance is reduced with compliant interlayers. The plates are set to the required mean temperature and difference, steady state is awaited and the heat flux recorded. The client specifies dry or moist condition, the mean temperature and whether the result is needed for a declared value or for a design conversion under EN ISO 10456.

    What the report states

    The report states thermal resistance R in m²·K/W and thermal conductivity λ in W/(m·K) at the mean temperature, together with density, thickness, moisture content by mass or volume and how contact resistance was handled. For moist tests the moisture content before and after is given so the value can be converted to other states using moisture conversion coefficients. Dry values commonly become the basis for tabulated design conductivities.

    Where the result is required

    EN 12664 supplies measured conductivities for masonry units and mortars under EN 1745, for gypsum products, wood-based panels, screeds, flooring, plastics and rubbers, and for any product too conductive for EN 12667. It supports thermal calculations under EN ISO 6946 and EN ISO 10456, EPD and product data sheets, and the thermal part of ETAs for wall kits and composite elements. Low-density insulation is tested under EN 12667 or EN 12939 instead.

    What we assess

    • thermal resistance (medium/low resistance)

    Products covered

    • thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre)
    • building materials

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    EN 12667 applies to specimens with a thermal resistance of at least 0.5 m²·K/W, which covers insulation products. Below that, in the range covered by the scope of EN 12664, contact resistance and specimen flatness control the error, and the extra provisions of EN 12664 are needed. Dense building materials nearly always fall under EN 12664.

    Yes, that is a specific purpose of the standard. The specimen is conditioned to the target moisture content, sealed against evaporation and tested quickly so that moisture redistribution under the temperature gradient stays small. The moisture content measured before and after the test accompanies the result; a dry reference value is still useful for conversions.

    Thick enough that the specimen's resistance clearly exceeds the contact resistances, yet within the apparatus limits and the heat-flow conditions of the standard. For concrete, mortar or masonry material a slab of several centimetres with ground, parallel faces is typical; the laboratory confirms dimensions for the chosen apparatus before samples are cast or cut.

    Related standards