    In short

    EN ISO 12570 - Hygrothermal performance of building materials - moisture content by drying at elevated temperature. Amstelfy's laboratory determines moisture content of thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre) and building materials according to EN ISO 12570 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 12570 determines

    EN ISO 12570 defines the moisture content of a porous building material as the mass of evaporable water it holds, determined by drying a specimen until its mass no longer changes. The drying temperature is chosen by material: 105 °C for materials that are stable at that temperature, 70 °C for those whose structure or composition changes between 70 and 105 °C, and 40 °C for materials such as gypsum that lose bound water or change above 40 °C. Constant mass is defined by a limit on the change between successive weighings a fixed time apart. The result is expressed as the ratio of water mass to dry mass, u, in kg/kg, and, with the density, as the moisture content by volume, ψ, in m³/m³. It is the reference quantity behind every moisture-dependent property, from thermal conductivity to sorption isotherms.

    Specimens, conditioning and procedure

    A specimen large enough to be representative is weighed in the state of interest, as delivered, after conditioning or after a thermal test, and placed in a ventilated drying oven at the temperature appropriate to the material; a desiccant is used where the standard prescribes it. Specimens are cooled to room temperature in a desiccator before each weighing so that the balance reading is not disturbed by convection. Weighing is repeated at intervals until the change between consecutive weighings is below the criterion of the standard, and the dry mass is recorded. If the volume moisture content is required, the specimen volume or the dry density is determined as well. The client indicates the drying temperature if the material has a known sensitivity, otherwise the laboratory selects it from the material class.

    What the report states

    The report states the initial and dry masses, the drying temperature, the moisture content by mass u in kg/kg or per cent, and where requested the moisture content by volume ψ, with the number of weighings to constant mass. The value serves as the reference moisture state for a thermal measurement, for conversion to other conditions with EN ISO 10456 coefficients, and as the dry mass for sorption testing.

    Where the result is required

    EN ISO 12570 is called up wherever a moisture state has to be defined: for the dry and moist specimens of EN 12664, as the starting point of sorption isotherms under EN ISO 12571, for moisture conversion of thermal conductivity under EN ISO 10456, for density of insulation and wood-based products at delivery, and for mass-balance checks in EPD data collection. Mineral wool, wood fibre, cellulose, aerated concrete, gypsum and mortars are frequent subjects.

    What we assess

    • moisture content

    Products covered

    • thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre)
    • building materials

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The standard groups materials by their stability: mineral and ceramic products dry at 105 °C, materials that soften, oxidise or lose volatile components between 70 and 105 °C dry at 70 °C, and materials that release bound water above 40 °C, such as gypsum, dry at 40 °C. The laboratory asks for the composition and chooses the lowest group that applies.

    Moisture by mass is easy to measure but misleading when comparing materials of very different density: a few per cent by mass in a dense concrete is much more water per cubic metre than the same figure in a light insulation. Thermal conductivity and sorption curves are therefore often given against moisture by volume, which needs the dry density of the specimen.

    It removes the evaporable water at the chosen temperature. Chemically bound water in hydrates stays in the material, and at 40 or 70 °C some physically bound water may remain as well. The value is therefore defined relative to the drying condition, which the report states, and comparisons between laboratories are valid only at the same temperature.

    Related standards

    All Thermal insulation products & hygrothermal test methods testing