Test method

    EN 826 – Compressive strength of insulation

    Thermal insulating products - compression behaviour

    Testing · NAC-037-TL

    In short

    EN 826 - Thermal insulating products - compression behaviour. Amstelfy's laboratory determines compressive stress at 10 % deformation / compressive strength of thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre) and building materials according to EN 826 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 826 determines

    EN 826 determines the compression behaviour of thermal insulating products. A square specimen of full product thickness is compressed between two parallel platens at a constant rate of displacement until it has been shortened by 10 % of its initial thickness, or until it fails earlier. From the force–deformation curve the standard derives either the compressive stress at 10 % deformation, σ10, when no yield occurs before that point, or the compressive strength, σm, when the curve passes through a maximum first. The distinction matters: rigid foams such as XPS or PIR often yield before 10 % and are characterised by strength, while mineral wool and most EPS grades deform progressively and are characterised by stress at 10 %. The compressive modulus can be evaluated from the linear part of the curve where the client requests it. Results describe short-term load capacity; sustained loads are covered separately by compressive creep testing.

    Specimens, conditioning and procedure

    Specimens are square prisms cut with faces parallel and at the product thickness, their side length set by the product standard or agreed with the client; the whole specimen area is loaded, so any facing or skin stays in place when it is part of the product. After conditioning, the specimen is centred between the platens of a compression machine, a pre-load of 250 Pa defines the zero of deformation, and the crosshead advances at 0.1 d per minute, where d is the specimen thickness in millimetres, until 10 % deformation or failure. Force and deformation are recorded continuously. Variants to agree are the specimen size, testing with or without skin for extruded products, the direction of loading for anisotropic products such as lamella boards, and whether the modulus is to be evaluated.

    What the report states

    Each specimen is reported with its compressive stress at 10 % deformation or its compressive strength, in kPa, together with the deformation at which the value was taken and, if requested, the compressive modulus in kPa. The mean of the set is compared with the level the manufacturer declares under the CS(10) family of codes, for example CS(10)100 for a minimum of 100 kPa, in which no single result may fall below the declared level.

    Where the result is required

    EN 826 is the method behind compressive stress or strength in EN 13162, EN 13163, EN 13164 and the other factory-made insulation standards, written CS(10)i or CS(10\Y)i depending on whether yield is allowed. The value governs the choice of insulation under floors, flat roofs, inverted roofs, perimeter and load-bearing applications, and it appears in ETICS assessments under EAD 040083 and in sandwich panel core characterisation related to EN 14509.

    What we assess

    • compressive stress at 10 % deformation / compressive strength

    Products covered

    • thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre)
    • building materials

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    If the force keeps rising up to 10 % deformation, the stress at that deformation is reported and no failure has occurred; this is typical for mineral wool and EPS. If the force reaches a maximum before 10 %, the specimen has yielded or crushed and the stress at that maximum is reported as compressive strength, which is common for XPS and rigid PIR.

    As delivered, unless the product standard or the application says otherwise. The skin stiffens the surface and raises the result, so a product sold with milled faces must be tested with milled faces. The report states the surface condition so that the value cannot be transferred to a different finish of the same foam.

    Only for short-term loading. Under a permanent load foams and mineral wool continue to deform by creep, and the design value for floors or inverted roofs is taken from compressive creep testing under EN 1606, which extrapolates long-term deformation at a fraction of the EN 826 stress. The 10 % value remains the classification parameter.

    Related standards

    All Thermal insulation products & hygrothermal test methods testing