Test method

    EN 12310-1 - Flexible sheets for waterproofing - resistance to tearing (nail shank) - bitumen sheets

    Testing · NAC-037-TL

    In short

    EN 12310-1 - Flexible sheets for waterproofing - resistance to tearing (nail shank) - bitumen sheets. Amstelfy's laboratory determines resistance to tearing (nail shank) of bitumen sheets according to EN 12310-1 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 12310-1 determines

    EN 12310-1 determines the resistance of bitumen waterproofing sheets to tearing at the shank of a nail, the way a mechanically fixed sheet or underlay fails when wind suction or sliding snow pulls it against its fastener. A nail of the shank diameter specified in the standard is driven through the specimen at a set distance from one edge; the sheet is gripped on the other side and pulled so that the nail shank is dragged towards the free edge. The maximum force before the nail tears through is the tear resistance in newtons. The result depends almost entirely on the carrier: polyester fleeces give high values, glass fleeces low ones. It is therefore the characteristic that tells a roofer whether a sheet can be nailed or must be bonded, and it is tested in both roll directions.

    Specimens, conditioning and procedure

    Rectangular specimens are cut in both the longitudinal and transverse direction, the number per direction following the standard. Each specimen is conditioned in the standard laboratory climate. A nail of the specified diameter is pushed through the specimen perpendicular to its plane at the prescribed distance from the free edge, and the specimen is clamped in the upper grip of a tensile machine while the nail is held in a bracket in the lower grip. The crosshead moves at the constant speed set in the standard until the nail has torn out through the edge. The maximum force is recorded for each specimen and the mean per direction is calculated, with the failure mode described.

    What the report states

    The report states the nail-shank tear resistance in N for the longitudinal and transverse direction, as the mean of the specimens with the individual values, and notes whether the carrier tore, delaminated or the nail cut cleanly through. Product standards require the manufacturer to declare the value, usually with a tolerance around the declared figure, in the Declaration of Performance.

    Where the result is required

    Cited by EN 13707 for mechanically fastened bitumen roofing sheets, by EN 13859-1 and EN 13859-2 for underlays nailed or stapled to rafters and studs, and by EN 13969 for damp proof sheets. Roofing guides set minimum nail tear values for underlays on counter-battens and for sheets fixed with washers, and wind-load calculations for mechanically fixed roofs start from this characteristic. Plastic and rubber sheets are tested by EN 12310-2.

    What we assess

    • resistance to tearing (nail shank)

    Products covered

    • bitumen sheets

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The nail shank concentrates the load on a few millimetres of carrier fibres; the bitumen coating adds little. Long-fibre polyester fleeces stretch and redistribute the load, so the tear force is high; glass fleeces are stiff and break fibre by fibre at low force. Reinforcing threads or scrims raise the value in the direction they run, which is why both directions are reported.

    The principle is the same, but EN 12310-2 for plastic and rubber sheets has its own specimen and loading arrangement suited to thin, extensible films, and results between the two parts are not compared. For underlays, EN 13859-1 and EN 13859-2 name EN 12310-1 for all materials so that roof underlays are rated on a common basis.

    The standard specifies a set of specimens for each roll direction, cut away from the roll edges and ends. A piece of sheet about one metre long across the full roll width covers both directions with spares for conditioning or retests. Send the product as sold, including any release film, which is removed before testing.

    Related standards

    All Waterproofing membranes, roof underlays & liquid-applied systems testing