Test method

    EN 1607 – Tensile strength of insulation

    Thermal insulating products - tensile strength perpendicular to faces

    Testing · NAC-037-TL

    In short

    EN 1607 - Thermal insulating products - tensile strength perpendicular to faces. Amstelfy's laboratory determines tensile strength perpendicular to faces of thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre) and building materials according to EN 1607 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 1607 determines

    EN 1607 measures how strongly an insulation product holds together across its thickness. A specimen is bonded on both faces to rigid plates, the plates are pulled apart in a tensile machine at constant speed and the maximum force at rupture divided by the specimen area gives the tensile strength perpendicular to faces, σmt. The property reflects fibre orientation and binder in mineral wool, bead fusion in EPS and cell structure in foams, and it is the characteristic that governs whether a bonded render, adhesive or membrane can be carried by the insulation without delamination within the board. Lamella mineral wool, with fibres standing perpendicular to the faces, reaches values an order of magnitude above standard slabs, which is why ETICS systems distinguish between the two. The method is a companion to EN 1608, which tests tensile strength parallel to the faces.

    Specimens, conditioning and procedure

    Square specimens of full product thickness are cut with faces parallel; the side length follows the product standard or the client's instruction. Each specimen is glued between two stiff plates with an adhesive that does not penetrate or soften the material, and the assembly is left for the adhesive to cure. In the tensile machine the plates are connected through self-aligning couplings so the load is axial, and the crosshead moves at 10 mm/min until the specimen separates. Force is recorded continuously and the failure surface is examined: rupture should occur inside the product; a break in the adhesive or at a facing is noted and such a result does not characterise the product. Conditioning, specimen size and testing of faced products with or without the facing are agreed beforehand.

    What the report states

    The report gives the tensile strength perpendicular to faces of each specimen in kPa, the mean of the set, the type of failure observed and the specimen dimensions. Manufacturers declare the level as TRi, for instance TR10 or TR80, meaning that no result lies below i kPa. For ETICS assessments the value is compared with the minimum the EAD sets for the insulation in the kit.

    Where the result is required

    The TR characteristic appears in EN 13162 for mineral wool and EN 13163 for EPS and in the other product standards for factory-made insulation. It is required for insulation used in bonded ETICS under EAD 040083, where the insulation must carry the base coat and render, for roof insulation under adhered waterproofing, and for sandwich panel cores, whose cross-panel tensile test in EN 14509 follows the same principle. Facade and roofing designers rely on it for wind-suction checks.

    What we assess

    • tensile strength perpendicular to faces

    Products covered

    • thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre)
    • building materials

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The adhesive must be stronger than the product and must not soak into it. If the plate separates at the adhesive before the product breaks, the force reached is only a lower bound and the result does not represent the material. The report records the failure type; the laboratory adjusts the adhesive or surface preparation and repeats on fresh specimens.

    In lamella products the fibres are oriented perpendicular to the faces, so the tensile load runs along the fibres and the binder bridges are loaded in shear. In a conventional slab the fibres lie mainly in the plane and the load pulls the layers apart. Density matters less than orientation, which is why ETICS specifications ask for lamellas or high-TR boards.

    The product standard fixes the number for a declared value and the laboratory follows it for an initial type test; for a development check a smaller set gives an indicative mean. Boards should be supplied uncut and at the thickness to be declared so that full-thickness specimens of the specified side length can be cut away from the edges.

    Related standards

    All Thermal insulation products & hygrothermal test methods testing