Test method

    EN 12086 – Water vapour transmission test

    Thermal insulating products - water vapour transmission properties

    Testing · NAC-037-TL

    In short

    EN 12086 - Thermal insulating products - water vapour transmission properties. Amstelfy's laboratory determines water vapour transmission / resistance factor of thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre) and building materials according to EN 12086 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 12086 determines

    EN 12086 determines how readily water vapour diffuses through an insulation product. A specimen is sealed over the mouth of a cup containing either a desiccant or a water or salt solution, creating a vapour pressure difference between the inside of the cup and the climate chamber in which the assembly stands. The assembly is weighed at intervals; once the mass change per unit time is constant, the water vapour transmission rate follows, and from it the permeance, the resistance, the permeability of the material and the dimensionless water vapour resistance factor μ, which compares the product with a layer of still air of the same thickness. The dry-cup and wet-cup arrangements represent different humidity ranges and can give different μ values for hygroscopic materials. The result decides how a product behaves in condensation calculations and whether it needs a separate vapour control layer.

    Specimens, conditioning and procedure

    Circular or square specimens of product thickness are cut to fit the cups, their thickness and area measured, and the edges sealed to the cup rim with wax or a sealant so that only the exposed face transmits. The cup is charged with desiccant for the dry-cup condition or with water or a saturated salt solution for wet-cup conditions, and placed in a chamber held at the temperature and humidity of the selected condition set. Weighings continue until successive rates of mass change agree within the limit of the standard. A correction for the air layer between the specimen and the desiccant or liquid is applied where the standard requires. Clients choose the condition set (dry cup or wet cup), the face to be exposed for faced products and whether the facing is included.

    What the report states

    The report states the water vapour transmission rate, permeance, resistance, permeability and resistance factor μ per specimen with the mean, the condition set used and the specimen thickness. For faced or thin products the water vapour resistance Z is reported directly. Manufacturers declare the factor as MUi or the resistance as Zi in the Declaration of Performance; the values enter Glaser-type and transient hygrothermal calculations.

    Where the result is required

    EN 12086 is the method named for water vapour transmission in EN 13162, EN 13163, EN 13164 and the other factory-made insulation standards, which either allow tabulated μ values or require measurement, and it supplies the sd value of insulation layers for condensation assessments under EN ISO 13788. Faced roof boards, ETICS insulation with vapour-tight finishes and wood fibre or cellulose products are typical subjects. Flexible sheets are tested under EN 1931 instead.

    What we assess

    • water vapour transmission / resistance factor

    Products covered

    • thermal insulation products (MW, EPS, XPS, PIR, PUR, wood fibre)
    • building materials

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    In hygroscopic materials such as wood fibre, cellulose or some facings, water adsorbed in the pores at high humidity opens additional transport paths, so permeability rises and μ falls under wet-cup conditions. Closed-cell foams show little difference. The report names the condition set, and the designer picks the value that matches the humidity range in the construction.

    The resistance factor μ describes a homogeneous material independent of thickness. When the product has a facing, a coating or layers that dominate the resistance, the factor is not meaningful and the product standards allow the measured water vapour resistance Z of the whole product to be declared instead, which is then used directly in the condensation calculation.

    For some materials the product standards provide tabulated values that may be declared without testing, generally conservative figures by density or thickness range. A manufacturer who wants to declare a more favourable or more precise value, or whose product carries a facing, has to measure it under EN 12086, and the test is also the check during product certification.

    Related standards

    All Thermal insulation products & hygrothermal test methods testing