Test method

    ISO 6272-2 - Paints and varnishes - rapid-deformation (impact resistance) tests - falling-weight test, small-area indenter

    Testing · NAC-037-TL

    In short

    ISO 6272-2 - Paints and varnishes - rapid-deformation (impact resistance) tests - falling-weight test, small-area indenter. Amstelfy's laboratory determines impact resistance of coatings of plastics, coatings, membranes, composites according to ISO 6272-2 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What ISO 6272-2 determines

    ISO 6272-2 is the small-area variant of the falling-weight impact test for paints and varnishes: a mass with a hemispherical indenter of 12.7 mm diameter falls from a chosen height onto a coated panel held over a die, and the coating in the deformed area is inspected for cracking and detachment. The smaller indenter concentrates the deformation, producing a deeper, sharper dent for the same energy than the 20 mm indenter of part 1, which emphasises the coating's ductility at the point of maximum strain and its adhesion around the dent. The method corresponds in geometry to the widely used ASTM D2794 Gardner-type tester, so it is the part chosen when results are to be compared with US data or with specifications written around that apparatus.

    Specimens, conditioning and procedure

    Panels are coated with the system under evaluation on the substrate named in the specification, usually steel of defined thickness, cured and conditioned. The panel is positioned on the die, coating towards the indenter for direct impact or away from it for reverse impact, and the weight is released from a known height. Either a fixed energy is applied at a number of positions and the coating is rated intact or cracked, or the height is varied in steps to locate the greatest energy without cracking. Inspection uses magnification and may be assisted by methods that reveal fine cracks. Film thickness, panel thickness, indenter and die dimensions and impact type are recorded for every result.

    What the report states

    The report gives impact energy in joules or the mass and height combination, direct or reverse impact, substrate and film thickness, the number of impacts and the proportion that remained crack-free, or the minimum cracking energy, with photographs of typical dents where useful. A comparison with the required value is stated when the client provides a specification.

    Where the result is required

    The small-area indenter test is used for coil and can coatings, powder coatings on metal furniture and façade panels, automotive and appliance finishes, and for coating systems whose specifications derive from ASTM D2794. In construction, EN 1504-2 and EN 13813 refer to the large-area part 1, so clients with concrete protection systems normally need that part; part 2 is requested for metal cladding and profile coatings, often together with cupping and bend tests.

    What we assess

    • impact resistance of coatings

    Products covered

    • plastics, coatings, membranes, composites

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    When the specification names the small indenter or ASTM D2794, when the coating is thin and hard, such as coil or powder coatings on metal, or when data must be compared with US test results. The two indenters produce different strain fields, so results from the two parts are not interchangeable.

    In reverse impact the coating is on the face that stretches, which exposes brittleness and poor adhesion that direct impact can mask. Many metal-coating specifications require the reverse impact value, because it predicts cracking at post-formed edges and bends of coated sheet.

    Several, at positions far enough apart and from the panel edges that the deformations do not interact; the standard sets the minimum spacing. For a determination of the cracking energy, more positions are needed as the step size is reduced around the transition, and a fresh panel is used when space runs out.

    Related standards