    ISO 6272-1 - Paints and varnishes - rapid-deformation (impact resistance) tests - falling-weight test, large-area indenter. Amstelfy's laboratory determines impact resistance of coatings of plastics, coatings, membranes, composites according to ISO 6272-1 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What ISO 6272-1 determines

    ISO 6272-1 determines the resistance of a coating to cracking or detachment when it is deformed rapidly by a falling weight. A guided mass with a hemispherical indenter of 20 mm diameter is dropped from a known height onto a coated panel resting on a die; the indenter deforms panel and coating together, and the coating is then examined for cracks and loss of adhesion. The large indenter spreads the deformation over a wider area than the small-area indenter of part 2, so the coating is strained more uniformly and the result discriminates between coatings mainly through their elasticity and adhesion rather than puncture resistance. Impact energy, the product of mass, gravity and drop height, is the variable; the test either checks a specified energy or finds the greatest energy the coating survives.

    Specimens, conditioning and procedure

    Coated panels of the substrate and thickness specified by the client, or steel panels prepared to the coating manufacturer's system, are conditioned and placed on the die of the falling-weight apparatus. The test may be run with the coating facing the indenter (direct impact) or facing away (reverse impact), and the report says which. For a pass/fail test the weight is dropped from the height corresponding to the required energy at several positions. For a determination, the height is increased or decreased in steps until the transition between intact and cracked coating is bracketed. After each impact the deformed area is examined under magnification for cracking and detachment, with the coating thickness measured next to the impact site.

    What the report states

    The report states indenter type and diameter, mass, drop height and energy in joules, direct or reverse impact, substrate type and thickness, coating thickness, number of impacts and the outcome per impact as crack-free or cracked, or the minimum energy at which cracking occurred. Where a class or requirement applies, conformity is stated against it.

    Where the result is required

    Impact resistance by this method is a declared characteristic of surface protection systems under EN 1504-2, with classes defined by impact energy, and of floor screeds and coatings in EN 13813, and it is used for powder and liquid coatings on steel, coil coatings and industrial floor finishes. For membranes and sheets the construction sector uses EN 12691, whereas thin automotive and can coatings are often tested with the small-area indenter of ISO 6272-2 or the US method ASTM D2794.

    What we assess

    • impact resistance of coatings

    Products covered

    • plastics, coatings, membranes, composites

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    Direct impact strikes the coated face and tests the coating in compression and spreading; reverse impact deforms the panel from behind and puts the coating in tension, which is more severe for adhesion and brittleness. Specifications for industrial coatings often require both, and the report identifies each result.

    The one that represents the application: for EN 1504-2 systems the coating is applied on the concrete substrate specified there; for metal coatings a steel or aluminium panel of defined thickness. Because the substrate deforms with the coating, results on different substrates are not comparable.

    The method is intended for coatings and thin systems that follow the deformation of the panel; thick elastic systems such as roof waterproofing are tested differently. Coating thickness is measured at each impact site and reported, because thicker films of the same material tend to crack at lower energy.