Test method

    EN ISO 13438 - Geosynthetics - screening test for oxidation resistance

    Testing · NAC-037-TL

    In short

    EN ISO 13438 - Geosynthetics - screening test for oxidation resistance. Amstelfy's laboratory determines oxidation resistance of geotextiles, geogrids and geocomposites according to EN ISO 13438 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 13438 determines

    EN ISO 13438 is the screening test for the resistance of polypropylene and polyethylene geosynthetics to oxidation. Polyolefins degrade by a chain reaction with oxygen that antioxidant additives hold back; once the stabilisers are consumed, strength falls quickly. The standard accelerates this by ageing specimens in air at elevated temperature in a ventilated oven, with separate conditions for polypropylene and polyethylene, or by exposing them to pressurised oxygen at a lower temperature, closer to the chemistry in the ground. After ageing the tensile strength is compared with that of unexposed specimens. A retained strength above the limit in the product standards qualifies the product for the standard durability statement of at least 25 years in natural soils with a pH between 4 and 9 and a temperature below 25 °C. EN 12447 covers hydrolysis of polyester and polyamide.

    Specimens, conditioning and procedure

    Specimens for ageing and their unaged references are cut from one sample. For the oven method the specimens are hung freely in a forced-ventilation oven at the temperature prescribed for the polymer, without touching each other or the oven walls, for the prescribed number of days, with temperature logged. For the pressurised method the specimens are sealed in an autoclave under oxygen at the prescribed pressure and temperature. After exposure the specimens are conditioned with the references and both sets are tensile tested, normally to EN ISO 10319. The method is chosen by polymer type, product thickness and the product standard's requirements; oxidative induction time of the raw material can be measured separately as a supporting indicator.

    What the report states

    Reported values are the mean tensile strengths of aged and unaged specimens with their scatter, the retained strength in percent, and the exposure record: method, oven temperature or oxygen pressure, and duration. Embrittlement, surface cracking or colour change seen on the aged specimens is described. Against the 50 % limit of the product standards the result either supports the 25-year durability statement or restricts the declared use, and the manufacturer transfers the outcome to the Declaration of Performance.

    Where the result is required

    The durability annexes of EN 13249 to EN 13257 and EN 13265 cite EN ISO 13438 for polypropylene and polyethylene geotextiles, geogrids and geocomposites, which includes most nonwoven geotextiles, tape wovens and drainage cores. Polymeric geosynthetic barriers of polyethylene use the related oxidation method EN 14575 under standards such as EN 13361. The test is used in CE marking, in product certification audits of durability claims and by designers specifying longer service lives in landfills and reinforced soil.

    What we assess

    • oxidation resistance

    Products covered

    • geotextiles
    • geogrids
    • geocomposites

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The two polymers oxidise at different rates and have different melting ranges, so the standard sets a temperature and duration for each that accelerates ageing without melting or distorting the specimen. Testing a polyethylene product under polypropylene conditions, or the reverse, would not give a result the product standards recognise.

    The oven exposes specimens to air at high temperature for weeks, which is quick but far from soil temperatures. The pressurised method uses pure oxygen at high pressure and lower temperature, so the degradation mechanism is closer to that in service and thick or heavily stabilised products are assessed more realistically. Both appear in the current edition.

    No. Oxidative induction time, measured by differential scanning calorimetry on the raw polymer, indicates how much antioxidant is present and is a useful factory control and research tool. The product standards require the retained strength after ageing to EN ISO 13438 for the durability statement; the two measurements are complementary.

    Related standards