Test method

    EN ISO 13433 - Geosynthetics - dynamic perforation test (cone drop test)

    Testing · NAC-037-TL

    In short

    EN ISO 13433 - Geosynthetics - dynamic perforation test (cone drop test). Amstelfy's laboratory determines dynamic perforation of geotextiles, geogrids and geocomposites according to EN ISO 13433 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN ISO 13433 determines

    EN ISO 13433 simulates the impact of a sharp stone dropped onto a geosynthetic during installation. A steel cone with a 45° point and a mass of 1000 g is released from a height of 500 mm onto a specimen clamped between rings of 150 mm internal diameter, and the diameter of the hole it makes is measured with a graduated measuring cone. A smaller hole means better resistance to dynamic perforation; a product that is not perforated is reported with a zero hole diameter. It is an index of survivability during placement rather than a design value, and complements the static puncture test: thick needle-punched nonwovens absorb the impact by stretching and give small holes, while stiff wovens of similar strength may split along the yarns and show larger openings. The result tracks mass per unit area and bonding.

    Specimens, conditioning and procedure

    Specimens are cut to EN ISO 9862 from positions across the laboratory sample and conditioned where required. Each is clamped flat and without slack in the ring assembly, the cone is positioned on the release mechanism with its tip 500 mm above the specimen surface, and released to fall freely through the guide. After impact the cone is removed and the measuring cone is lowered gently into the hole; the diameter is read from its scale after the settling time in the standard, without enlarging the hole. The procedure is repeated on each specimen of the set, and the condition of the cone tip is checked between tests. Wet testing can be performed for products used under water.

    What the report states

    The report gives the hole diameter in millimetres for each specimen, the mean and the coefficient of variation, and records specimens that were not perforated. The mean hole diameter is declared, with its tolerance, as the dynamic perforation characteristic in the Declaration of Performance. Specifiers use the value in survivability classes for separation and protection layers under coarse fill.

    Where the result is required

    Every harmonised geotextile standard from EN 13249 (roads) to EN 13265 (liquid waste) lists dynamic perforation among the characteristics to declare, and the geosynthetic barrier standards use it for membranes that receive aggregate directly. The value matters most where the fill is dropped or tipped onto the product: separation layers under road and railway sub-base, protection layers over geomembranes in landfills and reservoirs, filters under riprap placed by excavator, and working platforms on soft ground. Robustness classes in national guides are built on it together with the CBR force.

    What we assess

    • dynamic perforation

    Products covered

    • geotextiles
    • geogrids
    • geocomposites

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    That the cone did not pass through the specimen. The standard records such specimens with a zero hole diameter and they are included in the mean, so a product that is perforated on only some specimens shows a low average with high scatter. The report lists the individual values so the client can see this.

    A needle-punched nonwoven decelerates the cone by stretching and by fibre displacement, so the energy is absorbed over a wide area. A tape-woven fabric is stiff and the cone separates the tapes along their length, producing a slit that the measuring cone reads as a larger hole. Mass, polymer and structure all influence the result.

    Specifications and national guides group geotextiles into robustness classes based on dynamic perforation, CBR force and mass, and match each class to a fill type, stone size and compaction method. A smaller declared hole diameter allows coarser, sharper fill or heavier placing equipment without an additional protection layer.

    Related standards

    All Geotextiles & geosynthetics testing