Test method

    EN 13755 - Natural stone test methods - water absorption at atmospheric pressure

    Testing · NAC-037-TL

    In short

    EN 13755 - Natural stone test methods - water absorption at atmospheric pressure. Amstelfy's laboratory determines water absorption of natural stone according to EN 13755 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What EN 13755 determines

    EN 13755 measures how much water a natural stone takes up when it is immersed at atmospheric pressure until it stops gaining mass. Specimens are dried to constant mass, immersed gradually so that air can escape from the pores, and weighed at intervals until two successive weighings agree within the limit in the standard; the water absorption is the mass gain expressed as a percentage of the dry mass. The quantity reflects the open porosity that water can fill without pressure, which is the porosity that matters for frost damage, staining, efflorescence and the weight of wet cladding. It is lower than the open porosity by vacuum saturation from EN 1936, since atmospheric immersion leaves some pores air-locked, and it differs from the capillarity coefficient of EN 1925, which describes the rate of uptake rather than the total.

    Specimens, conditioning and procedure

    A set of specimens, normally six, is prepared as cubes or cylinders of the size permitted by the standard, with sawn faces and no visible defects. The specimens are dried in a ventilated oven at 70 °C to constant mass, cooled in a desiccator and weighed. They are then placed in a tank and water is added in stages, first to about half the specimen height, later to three quarters and finally to full immersion, with the waiting times given in the standard. At the prescribed intervals each specimen is removed, wiped with a damp cloth, weighed and returned, until constant mass is reached. Water absorption is calculated for each specimen from the saturated and dry masses.

    What the report states

    The report gives the water absorption at atmospheric pressure in percent by mass for each specimen, to one decimal place, with the mean and, where the product standard requires it, the standard deviation; dry density may be added when the dimensions are measured. The manufacturer declares the mean as the water absorption characteristic in the Declaration of Performance under the natural stone product standards, and specifiers use it to compare stones and to set cleaning and sealing regimes.

    Where the result is required

    Water absorption at atmospheric pressure is a declared characteristic in the harmonised natural stone standards: EN 1469 for cladding slabs, EN 12057 for modular tiles, EN 12058 for floor and stair slabs, EN 1341, EN 1342 and EN 1343 for external paving, and EN 771-6 for natural stone masonry units. It is also used to identify a stone type alongside the petrographic description, in heritage work to match replacement stone, and as a screening value before frost resistance testing to EN 12371.

    What we assess

    • water absorption

    Products covered

    • natural stone

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    EN 13755 gives the total amount of water a stone absorbs when fully immersed at atmospheric pressure, in percent by mass. EN 1925 measures the rate at which water rises into a stone by capillarity from one face, as a coefficient in g/(m²·√s). A stone can have a low total absorption but a high initial capillary rate, or the reverse.

    The standard allows cubes or cylinders within the size range it defines, and a set of six specimens is the usual number. Specimens can be cut from slabs, tiles or blocks supplied by the client; for stones with visible bedding or foliation the laboratory records the orientation, because absorption and the companion strength tests can differ with direction.

    Sudden full immersion traps air in the pore network and the stone cannot reach its true saturated mass. Raising the water level in steps lets air escape upwards through the dry part of the specimen, so the final mass is reproducible between laboratories. The staged timing is part of the standard procedure.