Test method

    ISO 4587 - Adhesives - tensile lap-shear strength of rigid-to-rigid bonded assemblies

    Testing · NAC-037-TL

    In short

    ISO 4587 - Adhesives - tensile lap-shear strength of rigid-to-rigid bonded assemblies. Amstelfy's laboratory determines lap-shear strength of adhesives, tile adhesives and tapes according to ISO 4587 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What ISO 4587 determines

    ISO 4587 is the international method for the apparent shear strength of an adhesive bond between two rigid adherends loaded in tension through a single-lap joint. It is the reference for comparing structural adhesives on metals and for process control in bonding operations, and it is the document with which the European method EN 1465 was aligned. The specimen has two flat adherends bonded over a 12.5 mm overlap and 25 mm width; the test records the force at failure and divides it by the bonded area. The standard restricts itself to rigid adherends, typically metal sheet of a standard thickness, because adherend deformation is part of the mechanics: a thinner or more flexible adherend lowers the apparent strength through increased peel at the overlap ends. Results are comparative, not design values.

    Specimens, conditioning and procedure

    Standard adherends are cut from the metal or rigid material agreed with the client, cleaned and surface-treated in a defined way because the preparation controls the bond quality as much as the adhesive does. The adhesive is applied to one adherend, the second is positioned with the overlap set by a jig, and the assembly is cured under the pressure, time and temperature of the manufacturer's instructions. After trimming any fillet and conditioning, each specimen is gripped so that the bond plane lies on the axis of loading, usually with spacers in the grips, and is pulled at a constant rate so that failure occurs within the time window of the standard. At least five specimens are tested.

    What the report states

    Apparent shear strength is reported in MPa for each specimen with the mean and standard deviation, the adherend material, thickness and surface preparation, bond line thickness where controlled, cure conditions, time to failure and the failure mode classified as adhesive, cohesive, substrate or mixed with the percentage of each. Where specimens were aged, retained strength as a percentage of the initial mean is added.

    Where the result is required

    ISO 4587 is cited in international and company specifications for structural adhesives, in aerospace and transport supplier qualification, in bonding process validation for metal and composite assemblies, and in ISO-based product standards outside the construction sector. Construction product manufacturers meet it when an export customer or an international adhesive specification names the ISO rather than the EN number, and in FRP strengthening and anchoring projects where adhesive characterisation follows ISO methods.

    What we assess

    • lap-shear strength

    Products covered

    • adhesives
    • tile adhesives
    • tapes

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The reference case is metal sheet of a standard thickness, commonly aluminium alloy or steel, but any rigid material that does not yield or fail before the adhesive can be used: rigid plastics, composites or wood-based panels. The adherend, its thickness and its surface preparation are reported, because results are only comparable between specimens with the same adherend configuration.

    The standard calls for a minimum of five specimens per condition, and more are advisable when the scatter is high or when the result will be used for a statistical acceptance limit. Specimens cut from a single bonded panel usually give lower scatter than individually bonded ones, because overlap and bond line thickness are more uniform.

    No. The single-lap specimen combines shear with peel and bending, so the apparent strength depends on the geometry and the adherends. Design values for bonded joints come from joint-specific testing or from thick-adherend and torsion methods that approach pure shear. ISO 4587 ranks adhesives, verifies processes and detects batch changes.

    Related standards

    All Rubber, elastomers, sealants & adhesives testing