Test method

    ISO 48-2 - Rubber, vulcanized or thermoplastic - hardness between 10 IRHD and 100 IRHD

    Testing · NAC-037-TL

    In short

    ISO 48-2 - Rubber, vulcanized or thermoplastic - hardness between 10 IRHD and 100 IRHD. Amstelfy's laboratory determines IRHD hardness of rubber compounds, elastomeric bearings and seals and waterstops according to ISO 48-2 under its ISO/IEC 17025 accreditation (NAC-037-TL). The method is typically part of initial type testing, ETA test programmes or factory production control verification; results are reported in English for manufacturers across Europe.

    What ISO 48-2 determines

    ISO 48-2 measures hardness in International Rubber Hardness Degrees. A rigid ball is pressed into the test piece first under a small contact force and then under a larger total force, and the additional depth of penetration is converted to IRHD through a relationship derived from the elastic modulus of a rubber. The scale was constructed so that 0 IRHD represents a material of zero modulus and 100 IRHD an infinitely hard material, and over the middle range the hardness is closely related to Young's modulus for an ideal elastic rubber. Four methods cover the range: the normal test N, the high-hardness test H, the low-hardness test L, and the micro test M, which is a scaled-down version for thin or small test pieces.

    Specimens, conditioning and procedure

    The test piece should have flat parallel faces and the thickness the method requires; the normal test uses pieces around 8 to 10 mm thick, which may be built up from thinner layers of the same material, while the micro test uses thin pieces of about 2 mm. After conditioning, the piece rests on a flat support under the instrument, the contact force is applied and the gauge is zeroed, the total force is added and the reading is taken after 30 seconds. Measurements are made at several points not closer to the edges or to each other than the method allows, and the median is reported. Instruments are verified against the dead-load reference method and reference blocks.

    What the report states

    Hardness is reported in IRHD, as the median of the readings with the method letter (N, H, L or M), test piece thickness, whether layers were plied and the conditioning applied. Where an apparent hardness is measured on a curved or non-standard piece the report says so. Changes after ageing or immersion are given in IRHD units against the initial median.

    Where the result is required

    IRHD is the scale used in EN 1337-3 for elastomeric bearings and in EN 681-1 for pipe and tunnel seals, in many bridge expansion joint and waterstop specifications, and in automotive and aerospace rubber component drawings. The micro method is the usual route for O-rings, thin seals and small mouldings. The result identifies the compound in type testing and certification files and anchors the ageing limits expressed as change in IRHD.

    What we assess

    • IRHD hardness

    Products covered

    • rubber compounds
    • elastomeric bearings and seals
    • waterstops

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030No
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    This test method is used inside initial type testing, ETA assessment programmes and factory production control verification. Amstelfy reports it as an accredited test under NAC-037-TL, either stand-alone or as part of a complete test programme.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    Yes - it is listed on the ISO/IEC 17025 testing scope NAC-037-TL.

    The micro test is for test pieces too thin or too small for the normal method, such as O-rings, thin gaskets and sections cut from small mouldings. It uses a smaller ball and smaller forces scaled so that the result approximates the normal test. Results from the two methods agree closely but not exactly, so the report states which was used.

    Rubber creeps under the indentor, so the penetration depth continues to increase slowly after the force is applied. Fixing the reading time at 30 seconds makes results reproducible between instruments and laboratories. A reading taken earlier would be higher, which is one reason IRHD and Shore values, read after a few seconds, do not coincide.

    ISO 48-2 uses a ball indentor under a fixed force increment and a 30 second reading, giving IRHD on a scale tied to the elastic modulus. ISO 48-4 uses a spring-loaded cone or truncated-cone indentor read after a few seconds, giving Shore A or D. IRHD is specified for bearings and seals; Shore dominates compound data sheets and profiles.

    Related standards

    All Rubber, elastomers, sealants & adhesives testing