European Assessment Document

    EAD 120109-00-0107 - Nosing expansion joints for road bridges

    Testing · NAC-037-TLCertification · NAC-026-PPSETA route

    In short

    EAD 120109-00-0107 is the EOTA European Assessment Document for nosing expansion joints for road bridges. Amstelfy Technical Solutions tests bridge expansion joints against this EAD in its ISO/IEC 17025-accredited laboratory in Amstelveen (NAC-037-TL): load-bearing capacity (static and fatigue), movement capacity, watertightness and durability of elastomer and steel components. The test reports follow the EAD clause structure so a Technical Assessment Body can use them directly for the European Technical Assessment; Amstelfy does not issue ETAs itself. Within its ISO/IEC 17065 scope (NAC-026-PPS) Amstelfy can also act as the product certification body for this product family.

    What the EAD assesses

    EAD 120109-00-0107 covers nosing expansion joints, the single-gap joint type in which steel or polymer-concrete nosings anchored to both deck edges hold a preformed elastomeric sealing element across the gap. Traffic runs over the nosings and the gap is closed only by the seal, so the joint is limited to the movement one flexible profile can accommodate, and its performance depends on three things: the anchorage of the nosings under wheel loads, the fatigue life of the nosing-to-deck connection, and the tightness and durability of the seal and its clamping. The EAD, which follows the ETAG 032 structure, defines the essential characteristics accordingly: mechanical resistance under static and fatigue loading, movement capacity, watertightness, resistance to wear and skid, durability of the elastomer and steel, and noise and drainage where claimed.

    Assessment programme

    A full-width joint segment with its anchorage is installed in concrete blocks. Static tests apply the vertical and horizontal wheel loads derived from the traffic load model of the Eurocode at the joint positions, checking deformation and anchorage. Fatigue loading repeats a reduced wheel load for the number of cycles set in the EAD on the nosing and its fixings, followed by inspection for cracks. Movement capacity is demonstrated by opening and closing the gap to the declared extremes, recording the force needed and checking the seal remains seated. Watertightness is tested with water standing over the joint at several gap openings. Elastomer durability uses the material tests for ageing, ozone, low temperature and chemical resistance referenced in the EAD.

    What the report states

    The report states the declared movement range in the longitudinal, transverse and vertical directions and the measured reaction forces; the static load capacity with deformations and residual deformation of the nosings; the fatigue outcome by inspection of the anchorage and seal after the cycle count; watertightness as pass or fail per gap position; wear and skid results; and the elastomer and steel durability data. The TAB uses them directly for the ETA performance tables.

    Where the result is required

    Nosing joints are the usual choice for short and medium spans with movements of a few tens of millimetres, on motorway overpasses, viaduct abutments and refurbishments where the existing recess is shallow. The ETA supports the road authority approvals that most European countries require for bridge joints, and the elastomer data feed national maintenance specifications. Where movement exceeds what one seal can take, designers move to modular joints under EAD 120113, and where traffic runs on the elastomer itself to mat joints under EAD 120110.

    What we assess

    • load-bearing capacity (static and fatigue)
    • movement capacity
    • watertightness
    • durability of elastomer and steel components
    • skid resistance and noise (where claimed)

    Products covered

    • bridge expansion joints

    Accreditation status

    ActivityStandardAccreditationValidityOn scope
    TestingISO/IEC 17025:2017NAC-037-TLvalid until 2 December 2028Yes
    Product certificationISO/IEC 17065:2012NAC-026-PPSvalid until 31 January 2030Yes
    Validation & verificationISO/IEC 17029:2019NAC-006-VVvalid until 31 January 2030No

    Route to market

    Products covered by an EAD are placed on the EU market with a European Technical Assessment issued by a Technical Assessment Body (TAB), followed by the AVCP tasks of a Notified Body and the manufacturer's Declaration of Performance and CE marking. Amstelfy performs the assessment tests, prepares the test reports in the EAD's clause structure and coordinates the test plan with the TAB; Amstelfy does not issue ETAs.

    How it works

    1. 1

      Send the standard number, product description and intended use

    2. 2

      We confirm the applicable test series, sample quantities and timeline

    3. 3

      Samples are delivered to Veilmeesterweg 20, 1187 ZW Amstelveen (Mon-Fri 09:00-17:00)

    4. 4

      You receive the report in English, written for the TAB, Notified Body, evaluation service or programme operator.

    Frequently asked questions

    No. ETAs are issued by Technical Assessment Bodies designated under the CPR. Amstelfy carries out the assessment tests in its accredited laboratory, prepares the test reports to the EAD's clause structure and coordinates the test plan with the TAB of your choice.

    A joint segment of the width specified in the EAD with its anchorage system, seals from the production range to be declared, installation instructions, and the elastomer compound data. Anchor layout and concrete class are agreed in advance so the test blocks match the manufacturer's installation detail.

    The elastomer is characterised as a material: hardness, tensile properties, compression set, accelerated heat ageing, ozone resistance and low-temperature behaviour, so that the seal can be replaced with the same compound during the service life. The seal retention in the nosing is tested on the assembled joint.

    When the manufacturer's kit includes the nosing material, its compressive and flexural strength, bond to the deck concrete and durability are assessed within the programme; where the nosing is a steel profile, the ETA covers the profile and the anchorage and the installer provides the material certificates.

    Related standards

    All Bridge expansion joints & structural bearings testing